Mechanical Properties Metric English Comments
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
PolyMirae Moplen RP343N Injection Molding Grade Polypropylene
Moplen RP343N is the polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP343N is a random copolymer particularly suitable for injecti..
Flexural Modulus 1.28 GPa
185 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Phillips 66 COPYLENE® CR027 Polypropylene, Homopolymer, Mini-random, BOPP
Mini-random homopolymer. Applications: BOPP film. Equivalent to Pro-fax® HL456JInformation provided by Phillips 66.
Flexural Modulus 1.28 GPa
185 ksi
0.05 in/mm, 1% Secant, Procedure A; ASTM D790
Phillips 66 COPYLENE® CM200LN-02 Polypropylene Impact Copolymer
COPYLENE™ CM200LN-02 is specially designed for injection molding applications where an excellent balance of stiffness/impact and good cycle times are required.Applications: Injection molding applic..
Flexural Modulus 1.27 - 1.76 GPa
185 - 256 ksi
Average value: 1.47 GPa Grade Count:5
Overview of materials for Polychlorotrifluoroethylene; Molded
This property data is a summary of similar materials in the MatWeb database for the category "Polychlorotrifluoroethylene; Molded". Each property range of values reported is minimum and maximum valu..
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
Hyosung Topilene J340F PP
J340F Film Grade Impact CopolymerApplications: Retort CPPCharacteristics:ProcessabilityHigh impactInformation provided by Hyosung Corporation
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
Hyosung Topilene J351F PP
J351F Block CopolymerApplications: Retort CPPCharacteristics:Excellent impact strengthFish eye freeHeat resistanceGood clarityInformation provided by Hyosung Corporation
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
Hyosung Topilene J740 PP
J740 Injection Impact CopolymerApplications: Large articles:Washing M/C partsElectric applianceIndustrial applianceCharacteristics:Medium impactFlowabilityInformation provided by Hyosung Corporation..
Flexural Modulus 1.27 GPa

@Thickness 6.40 mm
185 ksi

@Thickness 0.252 in
30mm/min; ASTM D790
LG Chemical LUPOL EI5002L PP
Description: Injection Molding, PP, General PurposeApplication: Automotive Interior PartsCAS: 9003-07-0 and 9002-88-4Information provided by LG Chemical
Flexural Modulus 1.28 GPa
185 ksi
ASTM D790B
Ineos L12Z-01 Polypropylene Impact Copolymer
Grade L12Z-01 is a nucleated and antistatic polypropylene copolymer with a medium melt flow rate that provides an excellent balance of stiffness and impact. It is especially formulated to help provi..
Flexural Modulus 1.27 GPa
185 ksi
ASTM D760
LG Chemical SEETEC M1400 Polypropylene Impact Copolymer
Features: SEETEC M1400 is a heterophasic polypropylene copolymer for injection molding applications. SEETEC M1400 exhibits a high flowability and a good balance of stiffness and impact strength. SEE..
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
LG Chemical SEETEC PB283 HDPE
Features: This high molecular weight, hexane copolymer is tailored for light-weight blow-molded containers that require: Good stiffness and Excellent processabilityAdditives: Anti-OxidantsApplicatio..
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
LG Chemical SEETEC PH162 HDPE
Features: Characteristics : Good balance of toughness & stiffness stressAdditives : Anti-Oxidants, LubricantsProcessing recommendations : Maintain the stock temperature 200-230°C (392-446°C) f..
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
LG Chemical SEETEC PM360 HDPE
Features: Characteristics: Excellent processability, Good tenacity & knot strengthAdditives: Anti-oxidants, LubricantsApplication: Tarpaulin, Woven bags (Inflation)CAS No. 25213-02-9Information prov..
Flexural Modulus 1.28 GPa
185 ksi
ASTM D790
Multibase Multi-Flex® D 6606 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHeat StabilizedOzone ResistantProcessability, GoodUV Resistance, Good R..
Flexural Modulus 1.27 GPa

@Thickness 6.40 mm
185 ksi

@Thickness 0.252 in
10mm/min; ASTM D790
LG Chemical LUPOL TE5104 PP+Rubber+MF, High Impact
Description: Injection Molding, PP+Rubber+MF, High Impact, Good WeatherabilityApplication: Automotive Exterior (Bumper Fascia, Rear Bumper Step)Information provided by LG Chemical
Flexural Modulus 1.28 GPa
185 ksi
secant; ASTM D790
Spartech PP7120 Talc Filled High Impact Copolymer
Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech
Flexural Modulus 1.27 GPa
185 ksi
Shinil Chemical SHINSTAT PETG Electrostatic Control Polymer Sheet Grade
SHINSTAT is an Inherently Dissipative Polymer (IDP) compound which can discharge the electrostatic charge (ESD) effectively. Shinil has designed SHINSTAT using Shinil's patented IDP technology for ..
Flexural Modulus 1.27 GPa
185 ksi
Shinil Chemical SHINSTRA PA-66 Devlop Structural Polymer Window Strip
SHINSTRA is the product line of structural polymer compound which exhibits excellent physical, mechanical, and thermal properties. Shinil uses the state-of-the-art dispersion and blending technolog..
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
Samyang Trilen® 9550AC Polypropylene, General Purpose
Mechanical strength and thermal resistance are excellent.9550AC is a general purpose grade.Applications: ConnectorsInformation provided by Samyang.
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
SCG Chemicals EL-Leneâ„¢ H5818J High Density Polyethylene Injection Molding
Key Characteristics:Good processabilityHigh stiffnessHigh impact strengthBalanced properties between shrinkage and warpageOdorlessSafe for food contactRecommended Applications: General purpose inje..
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
SCG Chemicals EL-Leneâ„¢ H6105JU High Density Polyethylene Injection Molding
Key Characteristics:Good processabilityWide service temperatureHigh rigidityGood weathering resistance (UV stabilizer)Recommended Applications:Crates for soft drinks, bottles, pallet, garbage bins, ..
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
SCG Chemicals EL-Proâ„¢ P722JO Polypropylene Injection Molding
Key Characteristics:Good flowabilityGood sealabilityGood mechanical property balanceMinimal shrinkage and warpageContains UV stabilizerRecommended Applications:Good impact automotive and electrical ..
Flexural Modulus 1.28 GPa
185 ksi
ASTM D790-90
Lubrizol Stat-Rite® S-250 Static Control Polypropylene
Stat-Rite® S-250 is a static dissipative Polypropylene alloy. Stat-Rite S-250 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD pr..
Flexural Modulus 1.28 GPa
185 ksi
ASTM D-790
CMT Materials REN Shape® 460 Prototype Tool & Precision Modeling Board
REN Shape 460 is a moderate density precision modeling board that features a lower coefficient of thermal expansion to provide enhanced dimensional stability over a broader temperature range than ot..
Flexural Modulus 1.28 GPa
185 ksi
1% secant, 0.05 in/min.; ASTM D790
ExxonMobil PP7684KN Impact Copolymer
Product Description: A high crystallinity, high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded small and large appliance ..
Flexural Modulus 1.28 GPa
185 ksi
ASTM D790
Amco PRIMATOP HDPE 004955HP Blow Molding Polyethylene
HDPE 003955PZ features zinc stearate additive and is used for injection blow molding.Former A-Top Polymers product; part of Amco product line since 2013.
Flexural Modulus 1.28 GPa
185 ksi
Tangent Method 1; ASTM D-790
Bapolene® 3255 Polyethylene, Injection Grade
Narrow molecular weight distribution injection molding resin. This resin offers good impact strength, resistance to warpage, and stiffness. This product meets the Food and Drug Administration requ..
Flexural Modulus 1.28 GPa
185 ksi
ASTM D-790
Bapolene® 4072 Polypropylene, Injection Grade
Bapolene PP4072 is a high flow, fast cycle injection molding resin. This product meets FDA standards for food contact applications.Applications: Appliances, containers, and thin-walled articles.Bap..
Flexural Modulus 1.27 GPa
185 ksi
ASTM D790
SCG Chemicals EL-Lene™ H6140B High Density Polyethylene Blow Molding
Key Characteristics:Good processabilityHigh stiffnessGood environmental stress cracking resistance (ESCR)High compressive and impact strengthExcellent appearanceOdorlessSafe for food contactGood pri..
Flexural Modulus 1.28 GPa
185 ksi
Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790
ExxonMobil Paxon™ AA50-002 Blow Molding Resin  (discontinued **)
AA50-002 is a blow molding grade high density polyethylene. This resin has excellent stress crack resistance combined with high impact strength, rigidity, and melt strength.Information provided by ..
Copyright © lookpolymers.com All Rights Reserved