Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

A. Schulman POLYFLAM™ E-17338 22% CACO3 Filled Copolymer Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 30% Calcium Carbonate (CaCO3) Filler
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman POLYFLAM™ E-17338 22% CACO3 Filled Copolymer Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolyfort® E 17338 is a 22% filled copolymer polypropylene product. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 1.07 g/cc
1.07 g/cc
ASTM D792
Melt Flow 1.0 g/10 min
1.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.0 MPa
4060 psi
ASTM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 1.80 GPa
261 ksi
ASTM D790
Izod Impact, Notched 0.300 J/cm
0.562 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 95.0 °C
203 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °C
131 °F
ASTM D648