Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 1.28 GPa | 186 ksi | 1% Secant; ASTM D790 |
Multibase Multi-Pro® 2520 XU Black Polypropylene Forms:PelletsProcessing Methods:Injection MoldingInformation provided by Multibase |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
PolyOne Maxxam™ FR PP 401 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
PolyOne Maxxam™ FR PP 402 Polypropylene, Unspecified (PP, Unspecified) Maxxam™ FR flame-retardant polyolefin compounds and masterbatches meet stringent flammability performance requirements defined by industry agencies, including Underwriters Laboratories UL 94 V-2, V.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | Test Method I, Procedure B (chs speed 0.05 in/min); ASTM D790 |
Network Polymers NPP 50-0252 Description: High Density Polyethylene (HDPE) Blow Molding GradeInformation provided by Network Polymers Inc. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
NOVA Chemicals Novapol® HB-W952-A HDPE Extrusion Resin Molded Plaque Properties. Features: High molecular weight, excellent ESCR, impact strength, high rigidity.Applications: large-part blow-molding, trash cans, drums, jerry cans, fuel tanks.Data provi.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2907 HDPE Injection Molding Resin Features: High stiffness, maximum impact strength and toughness, good top loading capability, high surface gloss.Applications: Protective sports equipment, safety helmets, high impact custom molding.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
NOVA Chemicals Sclair® 2908, 2908-UV8A HDPE Injection Molding Resin Features: High stiffness, maximum impact strength and toughness.Applications: Tote boxes, beverage crates.Data provided by the manufacturer. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | 0.05 in/min; 1% secant; Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CR027 Polypropylene, Homopolymer, Mini-random, BOPP Mini-random homopolymer. Applications: BOPP film. Equivalent to Pro-fax® HL456JInformation provided by Phillips 66. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
PolyOne Edgetek® SY-15GB/000 Polystyrene (PS), Glass Bead Filled
(discontinued **) Description/Features:Glass Bead FilledUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
Chevron Phillips Marlex® HXM TR-570 High Density Polyethylene
(discontinued **) High Density PolyethyleneCustomer Benefits: This extra high molecular weight polyethylene is tailored for large containers with exhibit outstanding impact and creep resistance, excellent ESCR, and e.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
NOVA Chemicals Sclair® 69A HDPE Extrusion Resin
(discontinued **) Features: High tensile strength, better moisture barrier, better oil and solvent resistance, lower friction coefficient, lower brittleness temperature, better abrasion resistance, better temperature.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | 0.05 in/mm, 1% Secant, Procedure A; ASTM D790 |
Phillips 66 COPYLENE® CM200LN-02 Polypropylene Impact Copolymer COPYLENE™ CM200LN-02 is specially designed for injection molding applications where an excellent balance of stiffness/impact and good cycle times are required.Applications: Injection molding applic.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790A |
Ineos H03G-03 Polypropylene Homopolymer
(discontinued **) Suggested fabrication methods: ExtrusionFeatures: Ease of processingTypical applications: Oriented filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from inject.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D790 |
Honeywell Aegis™ PL75HS Medium Viscosity, Heat Stabilized, Flexible Nylon 6
(discontinued **) Description: Aegis PL75HS is a medium viscosity, heat stabilized, flexible nylon 6 especially suited to the production of extrusion profiles offering a combination of good flexibility, toughness and.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790A |
Ineos H03G-00 Polypropylene Homopolymer Suggested fabrication methods: ExtrusionFeatures: Low water carry-overTypical applications: Woven fabric, Cordage, Slit filmComplies with FDA specification, Title 21, CFR 177.1520.Typical property d.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | Tangent-Method; ASTM D790 |
Ineos T50-400 HDPE T50-400 is a high density polyethylene copolymer having a narrow molecular weight distribution. It is intended for injection molding applications where a good balance of processability and end-use p.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | secant; ASTM D790 |
Spartech PP7120 Talc Filled High Impact Copolymer Good material choice for applications where low to medium levels of impact are required and where stiffness and heat deflection properties remain criticalInformation provided by Spartech |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP 2Z004 ETFE LNP* THERMOCOMP* 2Z004 is a compound based on ETFE resin containing 20% Milled Glass. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp 2Z004 FP-E (EFTE) LNP* 2Z004 is a compound based on Ethylenetetrafluoroethylene (ETFE) containing Milled Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D790-90 |
Lubrizol Stat-Rite® S-250 Static Control Polypropylene Stat-Rite® S-250 is a static dissipative Polypropylene alloy. Stat-Rite S-250 utilizes the patented Stat-Rite® inherently dissipative polymer (IDP) alloy system to provide clean, permanent ESD pr.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | 3 pt. Tangent; ASTM D790 |
Chevron Phillips Marlex® 9004 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | 3 pt. Tangent; ASTM D790 |
Chevron Phillips Marlex® 9006 HDPE Injection Molding Resin Resin Type: Linear Copolymer, ASTM D 4976 Classification: PE 233, A 56700Characteristics: Moderate Flow, Excellent Impact Strength, Good Stiffness, Excellent ESCR, Moderate Shrinkage ResistanceAppli.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | |
CMW® ELKONITE® 3W53 Heat Treatable Tungsten Copper material For resistance welding electrodes.Information provided by CMW Inc. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | 1% secant, 0.05 in/min.; ASTM D790 |
ExxonMobil PP7684KN Impact Copolymer Product Description: A high crystallinity, high impact copolymer resin with medium melt flow rate and excellent processing attributes. It is designed for injection molded small and large appliance .. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D790 |
Amco PRIMATOP HDPE 004955HP Blow Molding Polyethylene HDPE 003955PZ features zinc stearate additive and is used for injection blow molding.Former A-Top Polymers product; part of Amco product line since 2013. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | Tangent Method 1; ASTM D-790 |
Bapolene® 3255 Polyethylene, Injection Grade Narrow molecular weight distribution injection molding resin. This resin offers good impact strength, resistance to warpage, and stiffness. This product meets the Food and Drug Administration requ.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | ASTM D-790 |
Bapolene® 4072 Polypropylene, Injection Grade Bapolene PP4072 is a high flow, fast cycle injection molding resin. This product meets FDA standards for food contact applications.Applications: Appliances, containers, and thin-walled articles.Bap.. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790 |
Albis Plastics Cellulose Acetate Butyrate B9004 (Odor Mask Added), 8% Plasticizer
(discontinued **) Amorphous Cellulose Acetate Butyrate (CAB)Characteristics: Dimensional Stability, Weatherability and Low Temp Impact StrengthApplications: Pens, Ski Goggles, Auto Trim, Skylights, Tool Handles and T.. |
|||
Flexural Modulus | 1.28 GPa | 185 ksi | Method1, Procedure A (1"x3"x0.125"), Tangent calculation; ASTM D790 |
ExxonMobil Paxon™ AA50-002 Blow Molding Resin
(discontinued **) AA50-002 is a blow molding grade high density polyethylene. This resin has excellent stress crack resistance combined with high impact strength, rigidity, and melt strength.Information provided by .. |
|||
Flexural Modulus | 1.28 GPa | 186 ksi | ASTM D790A |
BP Amoco Acctuf® 3434 Impact Copolymer Polypropylene
(discontinued **) Suggested fabrication methods: Injection moldingFeatures: High gloss, Nucleated, AntistaticComplies with FDA specification, Title 21, CFR 177.1520.Typical property data below from injection molded s.. |