Bapolene® 3042U Polyethylene, Rotational Molding Grade

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE
Manufacturer Bapolene®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolene® 3042U Polyethylene, Rotational Molding Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolene 3042U is a hexene linear low density polyethylene designed to provide an excellent combination of ESCR and impact. It contains a UV additive package and complies with US FDA 21CFR177.1520.Applications: Trash bins, large industrial and chemical storage containers, and drums.All data is based on molded plaques.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
ASTM D-1505
ESCR 100% Igepal® 1000 hour
1000 hour
>1,000; ASTM D-1693
Melt Flow 5.5 g/10 min
5.5 g/10 min
ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.0 MPa
2470 psi
ASTM D-638
Flexural Modulus 0.872 GPa
126 ksi
ASTM D-790
Descriptive Properties Value Comments
Process Rotational Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution