Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.869 GPa | 126 ksi | Tangent; ASTM D790 |
Flint Hills P9M6K-041A Specialty Impact Copolymer Polypropylene Features: Good clarity and impact resistance. Product does not contain animal derived components.Applications: Injection molding - durable goodsInformation provided by Flint Hills Resources. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE LNP* STAT-KON* FX98500 is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE (Asia Pacific) LNP* Stat-kon* FX98500C is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 0.869 GPa | 126 ksi | ASTM D790 |
Sterigenics Raprex® R100D Branched High Density Polyethylene Applications: ExtrusionRAPREX® R100D is a high density polyethylene based resin that exhibits an excellent balance of melt processability and physical properties due to its unique branched struct.. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp TH0450D LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp TH0450D LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific) LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp TH0450D PUR (Asia Pacific) LNP* Thermocomp* TH0450D is a compound based on Polyurethane resin containing High Specific Gravity Filler. Added features of this material include: High Specific Gravity.This data was supplied by .. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON FX98500 PE (Asia Pacific) LNP* Stat-kon* FX98500 is a compound based on Polyethylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON FX98500C PE LNP* STAT-KON* FX98500C is a compound based on Polyethylene resin containing Proprietary Filler(s). Added feature of this material is: Electrically Conductive. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 2X00858 FP-F (FEP) LNP* THERMOCOMP* 2X00858 is a compound based on FEP resin containing proprietary fillers. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D790 |
UBE UBESTA® 3020IX1 Rigid Automotive Grade Nylon 12 Description: UBE UBESTA® Automotive grade Nylon 12Comments: conductive, impact modifiedInformation provided by UBE. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product DescriptionPolyfort® CFP 4611 is an 11% CACO3 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product DescriptionPolyfort® CFP 4611 is an 11% CACO3 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product DescriptionPolyfort® CFP 4611 is an 11% CACO3 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product DescriptionPolyfort® CFP 4611 is an 11% CACO3 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product DescriptionPolyfort® CFP 4611 is an 11% CACO3 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D790 |
A. Schulman POLYFLAM™ CFP 4611 11% CACO3 filled copolymer polypropylene product DescriptionPolyfort® CFP 4611 is an 11% CACO3 filled copolymer polypropylene product. Information provided by A. Schulman. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ISO 178 |
Ecomass® 1007TU78 Tungsten Filled COPA Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsTungsten Powder Filled Co-Polyamide (COPA)Excellent ToughnessInformation provided by Technical Polymers |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | ASTM D790 |
Covestro Baydur® 730 IBS Polyurethane Structural Foam RIM, Density 35 pcf, MDI-based 2-Component Liquid System 0.25 in. thickness. IBS = Interactive Blowing System RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience .. |
|||
Flexural Modulus | 0.869 GPa | 126 ksi | |
Dow DOWLEX™ IP-60 High Density Polyethylene DOWLEX® IP-60 resin is an improved processing high density polyethylene resin designed to offer excellent processability, good impact and top load strength required in thin wall injection molding. .. |
|||
Flexural Modulus | 0.870 GPa | 126 ksi | SAE J949 |
Azdel SuperLite® SL550600-100 PP Resin Matrix / 55% Glass Fiber (3 mm Molded Thickness) AZDEL SuperLite® SL550600-100 is a low pressure, thermoformable, thermoplastic composite of polypropylene and long chopped glass fibers. Usually combined with outer layers as needed for the applic.. |
|||
Flexural Modulus | 0.872 GPa | 126 ksi | ASTM D-790 |
Bapolene® 3042U Polyethylene, Rotational Molding Grade Bapolene 3042U is a hexene linear low density polyethylene designed to provide an excellent combination of ESCR and impact. It contains a UV additive package and complies with US FDA 21CFR177.1520... |
|||
Flexural Modulus | 0.868 GPa | 126 ksi | ISO 178 |
Breplast Bretene SP Polypropylene / Polyethylene Composite Recovered polypropylene and polyethylene compositeInformation provided by Breplast S.p.A. |