Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bapolan® 6409 Polystyrene, Injection Grade

Category Polymer , Thermoplastic , Polystyrene (PS)
Manufacturer Bapolan®
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bapolan® 6409 Polystyrene, Injection Grade.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Bapolan PS6409 is designed for injection molding applications requiring superior impact and gloss. It complies with US FDA21 CFR177.1640 and 94HB UL rating.Application: General purpose.Bapolene® and Bapolan® are registered trademarks of Bamberger Polymers, Inc. Information provided by Bamberger Polymers. All data is based on molded plaques.
Physical Properties Metric English Comments
Melt Flow 9.0 g/10 min
9.0 g/10 min
200'C/5,000g; ASTM D-1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 20.7 MPa
3000 psi
ASTM D-638
Elongation at Yield 52 %
52 %
ASTM D-638
Flexural Modulus, 1% Secant 2068 MPa
299900 psi
ASTM D-790A
Izod Impact, Notched 1.34 J/cm
2.51 ft-lb/in
@23'C; ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 87.0 °C
189 °F
ASTM D-648
Descriptive Properties Value Comments
Process Extrusion
Injection Molding
Region Europe/Turkey
Bamberger Polymers Distribution
International
Bamberger Polymers Distribution
Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Copyright © lookpolymers.com All Rights Reserved