Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics GELOY FXW710SK ASA General purpose injection molding ASA with Visual Fx sparkle effect. |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 500ECR PC Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a.. |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 500ECR PC (Asia Pacific) Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a.. |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics Lexan® 500ECR PC (Europe-Africa-Middle East) Lexan* 500ECR Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. It is of non-chlorinated & non-brominated flame retardant systems with UL-94 V0 rating at 2.3mm. It is a.. |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | 0.125 in.; ASTM D256 |
Resirene Resirene® READ 9500 Ignition Resistant Impact Polystyrene Features:High FlowIgnition ResistantNo Pre-drying RequiredHigh ImpactColors AvailableApplications:Injection MoldingDark ColorsTV CabinetsElectronic EquipmentInformation provided by US distributor Ca.. |
|||
Izod Impact, Notched | >= 1.34 J/cm | >= 2.51 ft-lb/in | Method A; ASTM D 256 |
Karina E-844-10/219-Y-ERYM White PVC Compound Tin stabilized PVC compound, recommended for extrusion of profiles for general applications. It is supplied in pellet form and should be processed at the temperature range of 170°C to 190°C.I.. |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
SABIC Innovative Plastics LNP THERMOCOMP RF006SXZ PA 66 LNP* THERMOCOMP* RF006SXZ is a compound based on Nylon 66 resin containing 30% Glass Fiber. Added feature of this material is: Heat Stabilized. |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
A. Schulman PP 1349 Polypropylene Medium Impact Copolymer Polypropylene DescriptionPolypropylene PP 1349 is a medium impact copolymer polypropylene.Information provided by A. Schulman. |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | @23'C; ASTM D-256 |
Bapolan® 6409 Polystyrene, Injection Grade Bapolan PS6409 is designed for injection molding applications requiring superior impact and gloss. It complies with US FDA21 CFR177.1640 and 94HB UL rating.Application: General purpose.Bapolene® a.. |
|||
Izod Impact, Notched | 1.34 J/cm @Thickness 3.17 mm |
2.51 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® 8234G HS 44% Glass Filled PA6 (Dry) Ultramid 8234G HS is a heat stabilized, 44% glass fiber reinforced polyamide 6 injection molding compound offering the highest level of strength, stiffness, high temperature performance and dimensio.. |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 528L-50G Nylon 66, 50% Glass Reinforced A general purpose 50% glass reinforced Nylon 66 resin.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 626SB Nylon 6 Copolymer A flexible nylon copolymer, heat stabilized, in black, for tubing and other extrusion applications.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 980LS-40G Nylon 612, 40% Glass Reinforced A 40% glass reinforced, heat stabilized Nylon 612 resin.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.34 J/cm @Thickness 3.17 mm |
2.51 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® B50L 01 PA6 (Dry) Ultramid B50L 01 is a high-viscosity, lubricated, general-purpose extrusion PA6 grade. It conforms to FDA requirements including, 21 CFR 177.1500,EU Directive 2002/72/EC, the German BfR recommendat.. |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® ABS 222 Medium impact, low flow, rigid with a matte finish. Suitable for injection molding and also extrusion for thin walls like refrigerator liners.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 1513 Polycarbonate A rigid flame retardant polycarbonate, UV stabilized in black for applications requiring superior dimensional stability and overall toughness.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 735LD Nylon 6 An impact modified, plasticized copolymer with improved impact resistance for injection molding.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.34 J/cm | 2.51 ft-lb/in | ASTM D256 |
Ashley Polymers Ashlene® 980LS-43GB Nylon 612, 43% Glass Reinforced A 43% glass reinforced, heat stabilized Nylon 612 resin in black.Data provided by the manufacturer |
|||
Izod Impact, Notched | 1.34 J/cm @Thickness 3.17 mm |
2.51 ft-lb/in @Thickness 0.125 in |
ASTM Test |
BASF Ultramid® B3GM35 BKQ642 23220 15/25% Glass/Mineral Filled PA6 (Conditioned) Ultramid B3GM35 BKQ642 23220 is a 40% combined glass-fiber and mineral reinforced, pigmented black injection molding PA6 grade. |