Indium Corp. Indalloy 157 Lead Solder Alloy

Category Metal , Nonferrous Metal , Lead Alloy , Solder/Braze Alloy
Manufacturer Indium Corporation of America
Trade Name Indalloy
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Indium Corp. Indalloy 157 Lead Solder Alloy.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information Provided by Indium Corporation
Physical Properties Metric English Comments
Density 10.96 g/cc
0.3960 lb/in³
Thermal Properties Metric English Comments
Melting Point 252 - 295 °C
486 - 563 °F
Solidus 252 °C
486 °F
Liquidus 295 °C
563 °F
Component Elements Properties Metric English Comments
Antimony, Sb 5.0 %
5.0 %
Lead, Pb 95 %
95 %