Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

BASF Capron® 8203C Nylon 6 (Conditioned)  (discontinued **)

Category Polymer , Thermoplastic , Nylon , Nylon 6 , Nylon 6, Unreinforced
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF BASF Capron® 8203C Nylon 6 (Conditioned)  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Capron 8203C is a high viscosity, nylon 6 extrusion compound, possessing a modified crystalline structure for increased property performance and faster set up for tubing and cable applications. It has high strength, stiffness and heat distortion temperature. It maintains excellent chemical resistance to greases, oils and hydrocarbons. It is available in natural, heat stabilized and pigmented versions.Capron 8203C is generally recommended for applications such as automotive tubing and cable liners.Data provided by Allied Signal.Processing: Max. water content 0.25%. Product is supplied in sealed containers and drying is not required. If drying becomes necessary, a dehumidifying or desiccant dryer operating at 85°C (185 °F). Is recommended. Drying time is dependent on moisture level.Melt Temperature: 240-280 degC (464-536 degF). Mold Temperature: 80-95 degC (176-203 degF). Injection and Packing Pressure: 35-125 bar (500-1500psi) A mold temperature of 80-95 degC (176-203 degF) is recommended, but temperatures of as low as 10 degC (50 degF) can be used where applicable. Injection pressure controls the filling of the part and should be applied for 90% of ram travel. Packing pressure affects the final part and can be used effectively in controlling sink marks and shrinkage. It should be applied and maintained until the gate area is completely frozen off. Fast fill rates are recommended to insure uniform melt delivery to the cavity and prevent premature freezing. Capron® is no longer a part of the BASF standard line. The BASF nylon products have been consolidated in the Ultramid ® line.
Physical Properties Metric English Comments
Density 1.13 g/cc
0.0408 lb/in³
(Dry)
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
ASTM Data MD (Dry)
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
ASTM test; 50 mm/min.
Elongation at Break >= 100 %
>= 100 %
Nominal
Elongation at Yield 15 %
15 %
ASTM test at 50 mm/min.
Flexural Yield Strength 30.0 MPa
4350 psi
ASTM Data
Flexural Modulus 0.840 GPa
122 ksi
ASTM Data
Thermal Properties Metric English Comments
Melting Point 220 °C
428 °F
(Dry)
Processing Properties Metric English Comments
Melt Temperature 240 - 280 °C
464 - 536 °F
Mold Temperature 80.0 - 95.0 °C
176 - 203 °F
temperatures as low as 10°C (50°F) can be used where applicable.
Drying Temperature 85.0 °C
185 °F
See Materials Notes
Injection Pressure 3.45 - 10.3 MPa
500 - 1500 psi
Copyright © lookpolymers.com All Rights Reserved