Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Axiall ProTherm® 4529 CPVC Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name PROtherm®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall ProTherm® 4529 CPVC Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf ProTherm® 4529 CPVC is a pelletized injection molding compound designed for large fittings. Typical applications are in potable water and chemical transfer systems especially where high resistance and/or elevated temperatures exist. 4529 has excellent processability, including thermal stability, flow, and surface appearance. ProTherm® 4529 is listed under NSF Standard 14 and Standard 61 and meets or exceeds ASTM D-1784 cell class 23447-B requirements.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.49 g/cc
1.49 g/cc
ASTM D-792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D-955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 117
117
ASTM D-785
Tensile Strength, Yield 62.1 MPa
9000 psi
ASTM D-638
Tensile Modulus 2.90 GPa
420 ksi
ASTM D-638
Flexural Strength 82.7 MPa
12000 psi
ASTM D-790
Flexural Modulus 2.69 GPa
390 ksi
ASTM D-790
Izod Impact, Notched 1.60 J/cm

@Thickness 6.35 mm
3.00 ft-lb/in

@Thickness 0.250 in
ASTM D-256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106.0 °C
222.8 °F
annealed; ASTM D-648
Deflection Temperature at 1.8 MPa (264 psi) 101.0 °C
213.8 °F
annealed; ASTM D-648
Descriptive Properties Value Comments
Cell Classification, ASTM D-1784 23447-B
Copyright © lookpolymers.com All Rights Reserved