Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D638 |
Plaskolite Optix® CA-68 General Purpose Acrylic Resin Injection Molding and Extrusion Grade. Good heat resistance, medium flow. |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D638 |
Quadrant EPP Nylatron® WP PA (ASTM Product Data Sheet) |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D638 |
Star Plastics ABSGF10 Molding Grade ABS With 10% Glass Information provided by Star Plastics, Inc. |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D638 |
Total PSC 500 Polystyrene Polystyrene 500 is a high melt, easy flow crystal polystyrene for fast cycle injection molding. The high flow characteristics of this material make it easy to fill thin parts. 500 is utilized in pro.. |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D-638 |
Axiall 9175 Amber 12 Rigid PVC, Molding, Amber 12 Georgia Gulf 9175 Amber 12 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It is a pre-colored amber compound.Information provided .. |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D-638 |
Axiall ProTherm® 4529 CPVC Rigid PVC, Molding Georgia Gulf ProTherm® 4529 CPVC is a pelletized injection molding compound designed for large fittings. Typical applications are in potable water and chemical transfer systems especially where hi.. |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D-638 |
Axiall SP-6340 Rigid PVC, Molding Georgia Gulf SP-6340 is a rigid vinyl injection molding compound designed for fittings and parts of similar confiation where maximum burst strength is required. Georgia Gulf 6340 is ideally suited .. |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D-638 |
Axiall 9175J Clear 38 Rigid PVC, Molding, Clear 38 Georgia Gulf 9175J Clear 38 is used for injection blow molding packages in cosmetic and toiletry applications such as hair dyes and shampoos. It has excellent clarity, flow and stability.Informatio.. |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D-638 |
Axiall MD-5009 Rigid PVC, Molding Georgia Gulf MD-5009 is a rigid, fitting-grade PVC compound designed for hot spruce/runner molds, large parts and multi-cavity molds. This compound is characterized by excellent processability, whi.. |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D638 |
Plaskolite West Optix® CA-68 General Purpose Acrylic Resin Injection Molding and Extrusion Grade. Good heat resistance, medium flow. |
|||
Tensile Modulus | 2.90 GPa | 420 ksi | ASTM D638 |
American Polymers API 392 Polystyrene API 392 is a general purpose polystyrene produced in pellet form for injection molding. API 392 has excellent clarity and high flow.Applications: Used in the manufacture of containers, housewares, .. |