Axiall 9153 Rigid PVC, Molding

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer Axiall
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Axiall 9153 Rigid PVC, Molding.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Georgia Gulf 9153 is an excellent combination of chemical resistance, impact and processing for chemically active products, such as pine oil cleaners.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.33 g/cc
1.33 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D-638
Tensile Modulus 2.59 GPa
375 ksi
ASTM D-638
Flexural Strength 76.5 MPa
11100 psi
ASTM D-790
Izod Impact, Notched 1.60 J/cm

@Thickness 6.35 mm
3.00 ft-lb/in

@Thickness 0.250 in
ASTM D-256
5.34 J/cm

@Thickness 3.17 mm
10.0 ft-lb/in

@Thickness 0.125 in
ASTM D-256
Tensile Impact Strength 168 kJ/m²
80.0 ft-lb/in²
ASTM D-1822
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F
ASTM D-648
Optical Properties Metric English Comments
Haze 6.0 %

@Thickness 3.17 mm
6.0 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Transmission, Visible 78 %

@Thickness 3.17 mm
78 %

@Thickness 0.125 in
pressed plaque; ASTM D-1003-61
Descriptive Properties Value Comments
Equilibrium Torque, meter-grams 1450
Brabender Plastograph, No. 6 Roller Head, 190°C Bath, 57-g. Charge; 60/43 rpm
Stability Time, minutes 30