Polymer Property : Tensile Strength, Yield = 6200 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D638
Omni Plastics OmniTuff™ HPP GRC10 MI30 Homopolymer Polypropylene Glass/Mineral Filled
Applications: Structural parts across industry segments including pump housings, wheels, handles, mountings, brackets, levers, pressure vessels, and furniture components.Information provided by Omni..
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D638
Polymer Resources PC/TP-FR3 Flame Retardant PC/Polyester Alloy
Flame Retardant, High Impact, Excellent Chemical ResistanceFeatures: • Flame Retardant • Impact Modified • Self Extinguishing • Good Chemical ResistanceProcess: Injection MoldingNotes: All p..
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D638
Ravago Manufacturing Americas Hylac® HF96 ABS
Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Rava..
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D638
I. Stern PS2110 General Purpose Crystal Polystyrene
Features:Moderately High Heat ResistanceUL Classification 94 HBExcellent Water ClarityApplicationsDisplaysHouse waresInformation provided by I. Stern & Co. Inc.
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM-D638
Ineos ABS Lustran® 427
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM-D638
Ineos ABS Lustran® 451 ABS, Injection Molding Grade
Lustran® ABS 451 is a soft flowing, medium impact injection molding resin designed with a unique balance of impact, heat resistance, flow, and gloss.
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D638
Spartech SP-9080 High Heat ABS Sheet
Description: ABS SheetInformation provided by Spartech.
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D 638
Styrolution PS 3600/3601 GPPS
Exceptional flow characteristicsGood for thin wall and complex partsUSP Class VI certifiedInformation provided by Styrolution
Tensile Strength, Yield 42.7 MPa

@Thickness 3.17 mm
6200 psi

@Thickness 0.125 in
ASTM D638
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 42.7 MPa

@Thickness 3.17 mm
6200 psi

@Thickness 0.125 in
ASTM D638
Samsung Cheil Industries Starex® SR-0340M High Heat Grade ABS
Information provided by Polymer Technology and Services, LLC (PTS).
Tensile Strength, Yield 42.7 MPa
6200 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS 7502
Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 42.7 MPa
6200 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS 9301
Description: Extrusion Grade, Low GlossInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 42.7 MPa
6200 psi
chs 2 in/min; ASTM D638
Diamond Polymers ASA TW-15H
Description: ASA Weatherable Polymer, Injection Molding Grade, High Heat Resistance, High IzodInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D638
Engineered Polymer Solutions ABS 550
Medium Impact. Natural and colors available. Medium gloss. Injection molding grade. Uses: General PurposeInformation provided by Engineered Polymer Solutions.
Tensile Strength, Yield 42.7 MPa
6200 psi
chs 2 in/min; ASTM D638
Diamond Polymers ABS 7501
Description: Injection Molding Grade, Extra High ImpactInformation provided by Diamond Polymers, Inc.
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D-638
Axiall 7450 Rigid PVC, Extrusion
Georgia Gulf 7450 is a special purpose rigid PVC extrusion compound designed for applications requiring the following properties: Excellent ToughnessSatin Surface AppearanceColorabilityChemical Res..
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D-638
Axiall SP-7221 Rigid PVC, Molding
Georgia Gulf SP-7221 is a high impact rigid vinyl compound designed for water distribution systems. The product is NSF listed under Standard 14.Information provided by Georgia GulfGeorgia Gulf beca..
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D-638
Axiall 2502 Rigid PVC, Extrusion
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D-638
Axiall 2506 Rigid PVC, Extrusion
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D-638
Axiall 7048A Rigid PVC, Extrusion
Georgia Gulf 7048A is a general purpose rigid PVC profile extrusion compound designed for applications requiring the following properties: Impact Strength & ToughnessFlame RetardantColorabilityCert..
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D-638
Axiall 9153 Rigid PVC, Molding
Georgia Gulf 9153 is an excellent combination of chemical resistance, impact and processing for chemically active products, such as pine oil cleaners.Information provided by Georgia GulfGeorgia Gulf..
Tensile Strength, Yield 42.7 MPa
6200 psi
ASTM D-638
Axiall 2503 Rigid PVC, Extrusion
Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.