Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 5.34 J/cm @Temperature 23.0 °C |
10.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Cycoloy® C1950 PC+ABS Low viscosity injection molding resin.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature 23.0 °C |
10.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Noble Polymers Regis™ 230106 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature 23.0 °C |
10.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Noble Polymers Regis™ 250107 Thermoplastic Olefin (TPO) Regis is a TPO (thermoplastic olefin) produced by Noble Polymers based on olefin/elastomer compounding. We have created Regis for use in bumpers and bumper fascias, air dams, exterior panels, materi.. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature -40.0 °C |
10.0 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PC-IM1 Polycarbonate, Impact Modified, Low Flow Polycarbonate, Impact Modified, Low FlowProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided .. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature -40.0 °C |
10.0 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Polymer Resources PC-IM1-UV Polycarbonate, Impact Modified, Low Flow, UV-stabilized Polycarbonate, Impact Modified, Low Flow, UV-stabilizedProcess: Molding or ExtrusionNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Inform.. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature -17.8 °C |
10.0 ft-lb/in @Temperature 0.000 °F |
ASTM D256 |
Polymer Resources PC-IM4 Polycarbonate, Impact Modified, Easy Flow Polycarbonate, Impact Modified, Easy FlowProcess: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.18 mm, Temperature -40.0 °C |
10.0 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-500-CX01 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature -30.0 °C |
10.0 ft-lb/in @Temperature -22.0 °F |
ASTM D256 |
Polymer Resources PC/ABS-GP1 General Purpose PC/ABS Alloy PC/ABS Alloy, General Purpose Process: Injection MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples.Information provided by Polymer Re.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
10.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lucent Polymers PC/ABS-1003 Polycarbonate+ABS, Extrusion / General Purpose, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
10.0 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Lucent Polymers PC/PBT-1420IM Polycarbonate+PBT, Superior Cold Temp Impact, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
10.0 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Lucent Polymers PC/PBT-1830 Polycarbonate+PBT, Superior Cold Temp Impact, Injection Grade Add "R" for Added ReleaseAdd "U" for UV StabilizerInformation provided by Lucent Polymers, Inc. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
10.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 GF4 IM L LE Availability: North AmericaForms: PelletsAdditive: Lubricant and Impact ModifierFeatures: Lubricant, Low Extractables and Impact ModifiedAppearance: Natural ColorInformation provided by TP Composite.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
10.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Elastoblend® PA6/6 IM5 BK Nylon 66 Availability: North AmericaForms: PelletsAdditive: Heat Stabilizer, Lubricant and Impact ModifierFeatures: Heat Stabilized, Lubricant and Impact ModifiedProcessing Method: Injection MoldingInformati.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
10.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Techmer ES Plastiblend® ABS/PA 1700 B1 Availability: North AmericaForms: PelletsAppearance: Natural ColorInformation provided by TP Composites, Inc. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature 23.0 °C |
10.0 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Noryl PX1404 PPE+PS PPE+PS blend. High Heat. FDA compliant with restrictions. Injection Molding and Extrusion.This data was supplied by SABIC-IP for the Americas region. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm, Temperature 22.8 °C |
10.0 ft-lb/in @Thickness 0.125 in, Temperature 73.0 °F |
ASTM D256 |
Lubrizol ISOPLAST™ 202EZ Engineering Thermoplastic Polyurethane Resin NSF Standard 61 CertifiedAvailable in Americas, Europe, Middle East, Africa, India and AsiaInformation provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
10.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D256 |
Diamond Polymers Centrex® 601 Profile Extrusion Grade AES Centrex 601 resin is a very high-impact, low-gloss AES (acrylonitrile-ethylene-propylene-styrene) resin with good resistance to weather aging. It has good melt strength for profile extrusion and can.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm, Temperature -30.0 °C |
10.0 ft-lb/in @Thickness 0.125 in, Temperature -22.0 °F |
ASTM D256 |
Diamond Polymers DIAMALOY PC 1113 Impact Modified Polycarbonate Information Provided by Diamond Polymers, Inc. & Network Polymers, Inc. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature 23.0 °C |
10.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256A |
Dow 334.03 Developmental Performance Polypropylene Polymer DOW D 334.03 Developmental Performance Polypropylene Resin is a propylene-based resin intended for use in extrusion blow molded containers requiring improved impact resistance. Targeted end-use app.. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature -40.0 °C |
10.0 ft-lb/in @Temperature -40.0 °F |
ASTM D256 |
Clariant Renol 6608-LLT Nylon 66, High Impact Modified, Lubricated, Low Temp Impact Data provided by Clariant Masterbatches |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 6.35 mm, Temperature 23.0 °C |
10.0 ft-lb/in @Thickness 0.250 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall CL-7049 Rigid PVC, Molding Georgia Gulf CL-7049 is a clear, high impact vinyl compound formulated for medical and food contact uses.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm, Temperature 23.0 °C |
10.0 ft-lb/in @Thickness 0.125 in, Temperature 73.4 °F |
ASTM D-256 |
Axiall MP-6585 Rigid PVC, Molding Georgia Gulf MP-6585 is an electrical grade rigid vinyl injection molding compound processing good strength, stiffness, toughness, and flow. In addition, it has excellent processing stability and s.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm, Temperature 0.000 °C |
10.0 ft-lb/in @Thickness 0.125 in, Temperature 32.0 °F |
ASTM D-256 |
Axiall SP-6655 Rigid PVC, Molding Georgia Gulf SP-6655 is a high flow rigid PVC compound designed for electrical and custom molding applications. This compound features excellent physical properties, good melt flow, and exceptional.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 6.35 mm |
10.0 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 9113 Rigid PVC, Molding Georgia Gulf 9113 is used for a variety of packages including charcoal lighter fluid, toiletries and household chemicals. It has excellent impact strength.Information provided by Georgia GulfGeorgi.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 6.35 mm |
10.0 ft-lb/in @Thickness 0.250 in |
ASTM D-256 |
Axiall 9113J Clear 13, 9113J Clear 61 Rigid PVC, Molding, Clear 13, Clear 61 Georgia Gulf 9113J Clear 13 and 9113J Clear 61 are used for a variety of packages including charcoal lighter fluid, toiletries and household chemicals. They have excellent impact strength and conta.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.17 mm |
10.0 ft-lb/in @Thickness 0.125 in |
ASTM D-256 |
Axiall 9153 Rigid PVC, Molding Georgia Gulf 9153 is an excellent combination of chemical resistance, impact and processing for chemically active products, such as pine oil cleaners.Information provided by Georgia GulfGeorgia Gulf.. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature 23.0 °C |
10.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Formosa Plastics Formolene® 6620A Impact Copolymer Polypropylene High Impact Copolymer for Injection Molding Formolene® 6620A is a copolymer of polypropylene designed and formulated for injection molding applications including pails, crates and furniture. It con.. |
|||
Izod Impact, Notched | 5.34 J/cm @Temperature 23.0 °C |
10.0 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
Formosa Plastics Formolene® 6630A Impact Copolymer Polypropylene Impact Copolymer for Injection Molding Applications Formolene® 6630A is a high impact copolymer of polypropylene designed and formulated for injection-molded applications. It contains a unique comb.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.18 mm, Temperature -20.0 °C |
10.0 ft-lb/in @Thickness 0.125 in, Temperature -4.00 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-100-CX02-EG PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |
|||
Izod Impact, Notched | 5.34 J/cm @Thickness 3.18 mm, Temperature -40.0 °C |
10.0 ft-lb/in @Thickness 0.125 in, Temperature -40.0 °F |
Injection Molded; ASTM D256A |
PolyOne Edgetek® XT XT-500-CX00 PC+PBT
(discontinued **) EDGETEK™ XT High Performance Polymers are polycarbonate and polyester alloys that combine strength, durability and chemical resistance. The Edgetek XT product family includes a complete line of gen.. |