Material Notes:
Georgia Gulf 9129J is designed for use in extruded price tag holders. The compound contains an ultraviolet light stabilizer which retards color change.Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013.
Physical Properties Metric English Comments
Specific Gravity 1.35 g/cc
1.35 g/cc
ASTM D-792
Mechanical Properties Metric English Comments
Hardness, Shore D 75
75
ASTM D-2240
Tensile Strength, Yield 46.9 MPa
6800 psi
ASTM D-638
Tensile Modulus 2.48 GPa
360 ksi
ASTM D-638
Flexural Strength 82.0 MPa
11900 psi
ASTM D-790
Flexural Modulus 2.41 GPa
350 ksi
ASTM D-790
Izod Impact, Notched 0.854 J/cm

@Thickness 3.17 mm,
Temperature 0.000 °C
1.60 ft-lb/in

@Thickness 0.125 in,
Temperature 32.0 °F
ASTM D-256
1.01 J/cm

@Thickness 3.17 mm,
Temperature 23.0 °C
1.90 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
ASTM D-256