Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 82.3 MPa | 11900 psi | ASTM D790 |
PolyOne Geon™ Vinyl Rigid Extrusion 87160 Polyvinyl Chloride, Rigid (PVC, Rigid) Note: NSF listings are obtained on specific colors. Contact PolyOne for the latest listing of approved colors for this product. Note: The Cell Classification was determined using the notched Izod te.. |
|||
Flexural Strength | <= 82.0 MPa | <= 11900 psi | ISO 178 |
Polykemi AB SCANBLEND FS7 UV4 PC/ASA Blend with Improved Weather Resistance Information provided by Polykemi AB |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790 |
PolyOne Geon™ Vinyl Fittings 210A White 271(HS) Polyvinyl Chloride, Rigid (PVC, Rigid) Information provided by PolyOne |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790 |
SABIC Innovative Plastics LNP FARADEX PS003E PA 6 (Asia Pacific) LNP* Faradex* PS003E is a compound based on Nylon 6 resin containing Stainless Steel. Added features of this material include: Electrically Conductive, EMI/RFI Shielding. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP KONDUIT PX08322 PA 6 LNP* Konduit* PX08322 is a compound based on PA6 resin containing mineral. Added features include: Thermally Conductive, Flame Retardant |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DL002P PC (Asia Pacific) LNP LUBRICOMP* DL002P is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Exceptional Processing. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | 2mm/min; ASTM D790 |
Kingfa JH950-602 Low-temperature Resistant & Flame Retardant PC/ABS Alloy Features:UL V-0 @ 3.2mmExcellent balance propertiesHigh heat resistanceGood normal/low temperature impact strengthGood surface, high glossApplications:ControllerPlug, socketShell of ammeterSmall hou.. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DL003E PC (Asia Pacific) LNP LUBRICOMP* DL003E is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Easy Molding. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP DL003P PC (Asia Pacific) LNP LUBRICOMP* DL003P is a compound based on Polycarbonate resin containing PTFE. Added features of this material include: Exceptional Processing. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP KAL22XXC Acetal Copolymer LNP* LUBRICOMP* KAL22XXC is a compound based on Acetal Copolymer resin containing 10% PTFE, 10% Aramid. Added feature of this material is: Wear Resistant. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OP005XXC PPS - LINEAR LNP LUBRICOMP* OP005XXC is a compound based on PPS - Linear resin containing 25% PTFE/Silicone. Added features of this material include: Wear Resistant. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRICOMP OP005XXC PPS (Asia Pacific) LNP* LUBRICOMP* OP005XXC is a compound based on Polyphenylene Sulfide resin containing PTFE, Silicone. Added features of this material include: Internally Lubricated. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY R2000 PA 66 LNP* LUBRILOY* R2000 is a compound based on Nylon 66 resin containing Proprietary Lubricant. Added feature of this material is: Wear Resistant. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790 |
Techmer ES HiFill FR® ABS GF20 FR RD073 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforcement, 20% Filler by WeightFeatures: Flame RetardantAppearance: RedInformation provided by TP Composites, Inc. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Valox® 357M PBT (Asia Pacific) This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON KD000 Acetal Copolymer (Europe-Africa-Middle East) LNP STAT-KON KD000* is also know as: LNP STAT-KON K, LNP STAT-KON KXC. It is a compound based on Acetal resin containing Carbon Powder. Added features of this material include: Electrically Conduct.. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp DX93681 PC (Asia Pacific) LNP* Thermocomp* DX93681 is a compound based on Polycarbonate resin containing Proprietary Filler(s).This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Strength | 82.0 MPa @Thickness 3.20 mm |
11900 psi @Thickness 0.126 in |
1.3 mm/min, Injection Molded; ASTM D790 |
Styron EMERGEâ„¢ 9500CR Polycarbonate (PC) / Polyethylene Terephthalate (PET) Overview: EMERGEâ„¢ PC/PET 9500 CR advanced resin is a polycarbonate blend with excellent chemical resistance and ignition resistance properties. This grade was designed for use in medical equipm.. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ISO 178 |
Styron Pulse® A35-105 PC/ABS PULSE™ A35-105 engineering resins give exceptional impact strength even at low temperatures and have high heat distortion temperature.Information provided by DowThis product line was spun off f.. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON RD000I PA 66 (Asia Pacific) LNP* STAT-KON* RD000I is a compound based on Nylon 66 resin containing Carbon Powder, Impact Modifier. Added features of this material include: Electrically Conductive, High Impact. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Xenoy® X5601WX PBT + PC + PET Impact modified PBT+PC+PET, Heat aging improved Xenoy |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790 |
Plenco 4414 Phenolic, Granular, Injection Molded PLENCO 04414 is a flock and mineral filled phenolic molding compound. It is formulated for use in electrical applications that require improved heat resistance, mechanical strength, and dimensional .. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790 |
Unitika L-1003PA Heat resistance, creep resistance, and excellent lubricantInformation provided by Unitika Ltd. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790 |
Unitika P-1001 Engineering Plastic P series resins are resins succeeding the characteristics of the neat polymer, U100, and improved in flowability and optical properties. Among many super engineering plastics, the resins are few tra.. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | GB/9341 |
Zhejiang Juner PC/ABS Alloy Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | Clear Casting |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Flexural Strength | 82.0 - 85.0 MPa | 11900 - 12300 psi | ASTM D790M |
DSM Somos® WaterClear® Ultra 10122 Optically Clear, Colorless, Rigid, Stereolithography Resin DescriptionDSM Somos® WaterClear Ultra 10122 is a next generation optically clear resin with ABS like properties and good temperature resistance. It produces colorless, functional, accurate parts .. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | ASTM D790, ISO 178 |
EPICHEM PA 6 Polyamide 6 Characteristics: medium viscosity, general purpose |
|||
Flexural Strength | 82.0 MPa | 11900 psi | dry; ISO 178 |
Azoty Tarnow™ Tarnamid® T-27 Polyamide 6 - Natural Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Tarnamid® has the following main properties:High mechanical strength, rigidi.. |
|||
Flexural Strength | 82.0 MPa | 11900 psi | GB/9341 |
Zhejiang Juner PC-3-1 Alloy Applications: Shell of Small Household Electric ApplianceInformation provided by Zhejiang Juner New Materials Co, Ltd. |