Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Atom Adhesives AA-DUCT CG2 Epoxy Adhesive

Category Polymer , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Atom Adhesives
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Atom Adhesives AA-DUCT CG2 Epoxy Adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AA-DUCT CG2 is a single component epoxy, formulated with silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulation. This concept opens the door to a wide range of applications previously prohibited by the much higher cost of Conventional silver conductive. AA-DUCT CG2 Formulated with Silver coated ceramic power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive substrates. AA-DUCT CG2 formulation produces electrically conductive paths on a wide variety of surfaces including plastics, rubber, cloth, thermoplastic, paper, wood and many others. AA-DUCT CG2 designed for use in diversified applications as microwave EMI & RFI shielding, in the assembly or repair of printed circuit boards, waveguides, electronic modules, flat cable, static shielding, connections, and circuitry.Appearance: Silver Coated ceramicCure Type: Heat cure Benefits: High strengthPerfect bondEMI & RFI shieldingWave guides Substrates: Excellent choice for the Integrated Circuits, aluminum, copper, magnesium, steel, bronze, nickel, kovar, ceramic, glass, phenolic and G-10 epoxy glass boards.Catalyst: AnhydrideInformation provided by Atom Adhesives
Physical Properties Metric English Comments
Viscosity 6800 cP
6800 cP
uncured
Mechanical Properties Metric English Comments
Modulus of Elasticity 4.14 GPa
600 ksi
Poissons Ratio 0.35
0.35
Shear Strength 13.8 MPa
2000 psi
cured
Adhesive Bond Strength 10.3 MPa
1500 psi
cured
Thermal Properties Metric English Comments
CTE, linear 57.0 µm/m-°C
31.7 µin/in-°F
cured
Specific Heat Capacity 0.300 J/g-°C
0.0717 BTU/lb-°F
cured
Thermal Conductivity 4.18 W/m-K
29.0 BTU-in/hr-ft²-°F
cured
Component Elements Properties Metric English Comments
Silver, Ag 65 - 75 %
65 - 75 %
ceramic
Electrical Properties Metric English Comments
Surface Resistivity per Square <= 0.10 ohm
<= 0.10 ohm
cured
Processing Properties Metric English Comments
Cure Time 42.0 min

@Temperature 200 °C
0.700 hour

@Temperature 392 °F
90.0 min

@Temperature 180 °C
1.50 hour

@Temperature 356 °F
150 min

@Temperature 160 °C
2.50 hour

@Temperature 320 °F
Pot Life 259200 min
259200 min
uncured
Shelf Life 6.00 Month
6.00 Month
uncured