Thermal Conductivity 4.18 W/m-K
29.0 BTU-in/hr-ft²-°F
cured
Atom Adhesives AA-DUCT CG2 Epoxy Adhesive
AA-DUCT CG2 is a single component epoxy, formulated with silver coated ceramic that results in lower material costs without adversely sacrificing the properties obtained with a pure silver formulati..