Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength, Yield | 46.0 MPa | 6670 psi | 50 mm/min; ISO 527 |
SABIC Innovative Plastics Cycolac® MG38 ABS Very high impact ABS. Toughness/rigidity. Good fatigue resistance. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | Type I, 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Cycolac® MG94 ABS (Asia Pacific) Superior flow, injection molding ABS. Good impact. For thin-wall applications. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | Type I, 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Geloy XTWE280 ASA (Europe-Africa-Middle East) Weatherble ASA profile extrusion gradeThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | 5 mm/min; ISO 527 |
SABIC Innovative Plastics LNP COLORCOMP WX96084 PBT (Europe-Africa-Middle East) LNP* COLORCOMP* WX96084 is a compound based on Polybutylene Terephalate resin. Added features include: Custom Color White. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | 50 mm/min |
Eastman Eastalloy DA106 PC+PET Copolyester/Polycarbonate
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | 50 mm/min |
Eastman Eastar DN102 PCTG Copolyester
(discontinued **) ISO data as provided by the manufacturer, Eastman Chemical |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | 50 mm/min |
Polimeri Europa SINKRAL G320 ABS
(discontinued **) Symbol according to ISO 1043-1: ABS Grade designation according to ISO 2580-ABS 1,MG,095-15-16-25 General purpose injection moulding grade with good impact resistance, good flow and high gloss. SI.. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | ISO 527 |
FKuR Kunststoff Bio-Flex® F 6611 Compostable PLA Blend The BIO-FLEX® trade name indicates blends of co-polyester and PLA* with, depending on the particular grade, a very high content of natural resource material. BIO-FLEX® does not contain any sta.. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | ISO 527 |
FKuR Kunststoff Biograde® C 6530 Biodegradable Plastic Compound BIOGRADE® are easy to process blends based on cellulose. BIOGRADE® is composed mainly of natural resources. Based on cellulose, a product of the paper industry BIOGRADE® has been especial.. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | |
Ineos ABS Lustran® H607AS Contains antistatic additives,Property data per ISO test methods. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | |
Ineos ABS Lustran® M203FC Standard impact strength, easy flowing, high gloss, BgVV and FDA quality for food contact. ,Property data per ISO test methods. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics NORYL STN15HF PPE+PS Automotive interiors. Improved flow characteristics/overall processing economy. 240F DTUL. High impact/good property retention after heat ageing. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP KP002 Acetal Copoly LNP* LUBRICOMP* KP002 is a compound based on Acetal Copolymer resin containing 10% PTFE/Silicone. Added feature of this material is: Wear Resistant. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | ISO 527 |
SABIC Innovative Plastics LNP LUBRICOMP ZL003 PPE+PS LNP* LUBRICOMP* ZL003 is a compound based on PPE+PS resin containing 15% PTFE. Added features of this material include: Wear Resistant. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X8303 PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized. For In Mold Decoration /Labeling. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics XYLEX X8303CL PC+POLYESTER (Europe-Africa-Middle East) PC+ POLYESTER, Transparent, Low processing Temperature, High flow with excellent impact, UV stabilized, OQ quality. For In Mold Decoration /Labeling. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | ISO 527 |
SABIC Innovative Plastics LNP THERMOCOMP KB003RXZ Acetal Copolymer LNP THERMOCOMP* KB003RXZ is a compound based on Acetal Copolymer resin containing 15% Glass Bead. Added features of this material include: Easy Release. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | 50mm/min; ISO 527-2 |
Styron Magnumâ„¢ 3513 Acrylonitrile Butadiene Styrene (ABS) MAGNUMâ„¢ 3513 is a grade which combines high impact with good flowability. It is suitable for injection molding and extrusion applications.Information provided by DowThis product line was spun .. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | Type I, 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP STAT-LOY SLWM2105 PBT+PC (Asia Pacific) Anti-static PBT/PC blend, mineral 5% filled product |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | ASTM D638 |
Eastman DuraStar MN620 Polymer, Natural Applications:Blood therapyDrug deliveryIV componentsMedicalSurgical instrumentsKey Attributes:Chemical resistance to most medical solvents including lipids and IPAProduct Description: DuraStar Poly.. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | ASTM D638 |
Eastman Eastar BR203 Copolyester Eastar BR203 Copolyester contains a mold release additive. It has excellent appearance and is nearly water-clear. Its most outstanding features are its chemical resistance and processing capabilitie.. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | ISO 527 |
Eastman Eastar MN004 Copolyester Eastar Copolyesters are brilliantly clear polymers that have excellent impact strength, chemical resistance, dimensional stability, and low shrinkage rates. Eastar MN004 contains a mold release.Appl.. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | ASTM D 638 |
Cossa Polimeri ESTADIENE 2020 MT Acrylonitrile Butadiene Styrene ABSMedium heat resistance, good impact resistance, good melt flow rate, high gloss, with antistatic, excellent processabilityInformation provided by Cossa Polimeri S.r.l. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | ASTM D638 |
Aclo Accucomp ABS ABS811L Medium Impact Grade |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | 50 mm/min |
Arkema Group Rilsan® AMN Y TLD Nylon 12, MoS2 Filled (Dry) Designation ISO 1874-PA12,MHLS,14-010,MD05Grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold-release agent.Low friction coefficient. Goo.. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | 50 mm/min |
Arkema Group Rilsan® BMN Y TLD Nylon 11, MoS2 Filled (Dry) Designation ISO 1874-PA11,MHLR,12-020,MD05Rigid grade with molybdenum filler for injection molding. Available color: steel gray. Light and heat stabilized. Mold release agent.No need of lubricant. L.. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | 2 in/min; ASTM Test |
BASF Ultramid® 8270 HS PA6 (Conditioned) Ultramid 8270 HS is a thermally modified PA6 blow molding compound exhibiting exceptional toughness and melt strength ideally suited for blow molding, profile extrusion, and other applications requi.. |
|||
Tensile Strength, Yield | 46.0 MPa | 6670 psi | ISO 527B |
Ineos Nova 212 Crystal Polystyrene Low Flow Grade
(discontinued **) Excellent balance of properties; Extrusion and Injection MoldingApplications: Foam insulation, XPS food packaging, Sheet and profile extrusion, CD and DVD jewel boxesProperties were determined on i.. |