Material Notes:
Basic Nylon 6, medium viscosity, lubricated with Molybdenum Disulfide.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Water Absorption 1.1 %
1.1 %
24 hrs; ASTM D570
Water Absorption at Saturation 8.0 %
8.0 %
ASTM D570
Linear Mold Shrinkage 0.011 cm/cm
0.011 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 120
120
ASTM D785
Tensile Strength, Ultimate 85.0 MPa
12300 psi
ATSM D638
Elongation at Break 60 %
60 %
ASTM D638
Flexural Modulus 2.70 GPa
392 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm
0.993 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 214 °C
417 °F
ASTM D3418
Deflection Temperature at 0.46 MPa (66 psi) 110 °C
230 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 93.0 °C
199 °F
ASTM D648