Material Notes:
A very high impact nylon resin for injection molding applications. Outstanding low temperature properties.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 1.5 %
1.5 %
ASTM D570
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 41.0 MPa
5950 psi
ASTM D638
Elongation at Break 85 %
85 %
ASTM D638
Flexural Modulus 1.60 GPa
232 ksi
ASTM D790
Izod Impact, Notched 9.10 J/cm
17.0 ft-lb/in
ASTM D256
2.10 J/cm

@Temperature -40.0 °C
3.93 ft-lb/in

@Temperature -40.0 °F
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D3418