Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polyram RamShine PV101 Acrylonitrile Butadiene Styrene

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Molded
Manufacturer Polyram
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polyram RamShine PV101 Acrylonitrile Butadiene Styrene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
General purpose ABS for injection molding applications.Information provided by Polyram.
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ISO 1183
Moisture Absorption at Equilibrium 0.22 %
0.22 %
50% RH; ISO 62
Water Absorption at Saturation 1.0 %
1.0 %
ISO 62
Linear Mold Shrinkage 0.0050 cm/cm
0.0050 in/in
ISO 2577
Melt Flow 18 g/10 min

@Load 10.0 kg,
Temperature 220 °C
18 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength, Yield 40.0 MPa
5800 psi
ISO 527
Elongation at Break 10 %
10 %
ISO 527
Tensile Modulus 2.30 GPa
334 ksi
ISO 527
Flexural Strength 65.0 MPa
9430 psi
ISO 178
Flexural Modulus 3.00 GPa
435 ksi
ISO 178
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ISO 75
Deflection Temperature at 1.8 MPa (264 psi) 100 °C
212 °F
ISO 75
Flammability, UL94 HB

@Thickness 3.00 mm
HB

@Thickness 0.118 in
Electrical Properties Metric English Comments
Volume Resistivity 1.00e+13 ohm-cm
1.00e+13 ohm-cm
IEC 60093
Surface Resistance 1.00e+13 ohm
1.00e+13 ohm
IEC 60093
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved