Ashley Polymers Ashlene® 62M Nylon 66, 40% Mineral reinforced

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, 40% Mineral Filled
Manufacturer Ashley Polymers
Trade Name Ashlene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Ashley Polymers Ashlene® 62M Nylon 66, 40% Mineral reinforced.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
A 40% mineral reinforced Nylon 66 resin modified for reduced shrinkage.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
ASTM D792
Water Absorption 0.070 %
0.070 %
ASTM D570
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength, Ultimate 83.0 MPa
12000 psi
ATSM D638
Elongation at Break 10 %
10 %
ASTM D638
Flexural Modulus 5.40 GPa
783 ksi
ASTM D790
Izod Impact, Notched 0.640 J/cm
1.20 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 257 °C
495 °F
ASTM D3418
Deflection Temperature at 1.8 MPa (264 psi) 121 °C
250 °F
ASTM D648