Material Notes:
A flexible nylon copolymer, heat stabilized, in black, for tubing and other extrusion applications.Data provided by the manufacturer
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
ASTM D792
Water Absorption 1.2 %
1.2 %
Linear Mold Shrinkage 0.014 cm/cm
0.014 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 43.0 MPa
6240 psi
ATSM D638
Elongation at Break 110 %
110 %
ASTM D638
Flexural Modulus 1.30 GPa
189 ksi
ASTM D790
Izod Impact, Notched 1.34 J/cm
2.51 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Melting Point 216 °C
421 °F
ASTM D3418