Material Notes:
AQUAMET 17 is a precipitation-hardening, martensitic stainless steel. Because it is hardened by a heat treatment, it provides high strength regardless of the diameter. It also offers good toughness and corrosion resistance. A popular choice, AQUAMET 17 is widely used in pleasure boats, ski boats, workboats, fishing trawlers, and crew boats, as well as pilot and patrol boats.Information provided by Crucible Specialty Metals.
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 931 MPa
135000 psi
Tensile Strength, Yield 724 MPa

@Strain 0.200 %
105000 psi

@Strain 0.200 %
Tension
Elongation at Break 12 %
12 %
in 2"; 8" to 12"
16 %

@Thickness <=203 mm
16 %

@Thickness <=8.00 in
in 2"
Reduction of Area 35 %

@Thickness 203 - 305 mm
35 %

@Thickness 8.00 - 12.0 in
50 %

@Thickness <=203 mm
50 %

@Thickness <=8.00 in
Shear Strength 483 MPa

@Strain 0.200 %
70000 psi

@Strain 0.200 %
Torsion
Component Elements Properties Metric English Comments
Carbon, C <= 0.070 %
<= 0.070 %
Chromium, Cr 14.5 - 16.5 %
14.5 - 16.5 %
Copper, Cu 3.0 - 5.0 %
3.0 - 5.0 %
Iron, Fe >= 70.903 %
>= 70.903 %
As Remainder
Manganese, Mn <= 1.0 %
<= 1.0 %
Nb + Ta 0.15 - 0.45 %
0.15 - 0.45 %
Nickel, Ni 3.0 - 5.0 %
3.0 - 5.0 %
Phosphorous, P <= 0.040 %
<= 0.040 %
Silicon, Si <= 1.0 %
<= 1.0 %
Sulfur, S <= 0.030 %
<= 0.030 %