Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Iran Petrochemical (PCC) 3840 UA Medium Density Polyethylene

Category Polymer , Thermoplastic , Polyethylene (PE) , MDPE , Medium Density Polyethylene (MDPE), Rotational Molded
Manufacturer Iran Petrochemical Commercial Co. (PCC)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Iran Petrochemical (PCC) 3840 UA Medium Density Polyethylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MD3840UA is a linear medium density polyethylene (MDPE) with butene copolymer. This polymer has good impact strength, excellent external and internal surface finish, whiteness, good stress cracking resistance, UV stabilized.Applications: rotational molded items with good stiffness, septic tanks, ordinary containers.Information provided by Iran Petrochemical Commercial Co.
Physical Properties Metric English Comments
Density 0.938 g/cc
0.0339 lb/in³
ASTM 1505-68
Environmental Stress Crack Resistance 400 hour
400 hour
ASTM D1693
Melt Flow 4.0 g/10 min

@Load 2.16 kg,
Temperature 190 °C
4.0 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238-7
Mechanical Properties Metric English Comments
Hardness, Shore D 65
65
ASTM D2240
Tensile Strength, Yield 15.0 MPa
2180 psi
ASTM D638-72
Elongation at Break >= 900 %
>= 900 %
ASTM D638
Flexural Modulus 0.650 GPa
94.3 ksi
ASTM D790
Charpy Impact, Notched 1.80 J/cm²
8.57 ft-lb/in²
ASTM D256
Thermal Properties Metric English Comments
Thermal Conductivity 0.480 W/m-K
3.33 BTU-in/hr-ft²-°F
ASTM D177
Vicat Softening Point 115 °C
239 °F
ASTM D1525
Processing Properties Metric English Comments
Melt Temperature 131 °C
268 °F
Copyright © lookpolymers.com All Rights Reserved