Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Strength | 24.0 MPa | 3480 psi | STN EN ISO 178 |
Plastcom PLASTALEN® EQ 18 N Polyethylene Impact modified PE for extrusion. Delivered in black color.Information Provided by Plastcom spol. s r.o. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
Ovation Polymers Nemcon™ E - PP AS Polypropylene, Anti-Static Nemcon™ E-Series products are designed for use in ESDA electronic assembly environments. E PP AS is a moisture independent anti-static polypropylene characterized by consistent moldability and recy.. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | after 24 hours at 350°C |
Pyrotek NAD-11 Structural Insulation Board NAD-11 is an asbestos-free cement board with excellent electrical properties. It has a high density cement board reinforced with inorganic fibers.ApplicationsCathode support pads Platen insulation .. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ASTM D790 |
SABIC M40060 Series High Density Polyethylene for Injection Molding Product Description: M40060 is a high density polyethylene grade with a narrow molecular weight distribution suitable for injection molding applications. It has been designed to provide good rigid.. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | 3.5%; ISO 178 |
GEHR Plastics PE-ELS® Polyethylene HDPE A variant of PE-HD with improved electrical conductivity.Polyethylene has a good chemical resistance against almost all acids and bases, detergents and hot water. PE has good insulation properties a.. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ASTM D790 |
LG Chemical LUPOL TE-5104K Thermoplastic Elastomer Alloy, 10% Polymer Alloy, High Modulus LUPOL resins, based on polyolefin with a wide range of characteristics, are a family of low cost engineering plastics.Applications: Automotive exterior parts.Information Provided by LG Chem |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added feature of this material is: Electrically Conductive. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON MD000 PP (Asia Pacific) LNP STAT-KON* MD000 is a compound based on Polypropylene resin containing Carbon Powder. Added features of this material include: Electrically Conductive. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 2Z004 ETFE LNP* THERMOCOMP* 2Z004 is a compound based on ETFE resin containing 20% Milled Glass. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-LOY M3000C PP LNP* STAT-LOY* M3000C is a compound based on unfilled Polypropylene resin. Added features of this grade include: Clean Compound System, Antistat. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
SABIC Innovative Plastics LNP Thermocomp 2Z004 FP-E (EFTE) LNP* 2Z004 is a compound based on Ethylenetetrafluoroethylene (ETFE) containing Milled Glass.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
Borealis Daplen™ EE340AE Polypropylene TPO Compound Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
Borealis Daplen™ EF261AI Polypropylene TPO Compound Daplen™ EF261AI is a 20 % mineral filled polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and is easy to process... |
|||
Flexural Strength | 24.0 - 30.0 MPa | 3480 - 4350 psi | ASTM D790M |
DSM Somos® 9420 Epoxy Resin for Stereolithography DescriptionDSM Somos® 9420 is a liquid photopolymer that produces robust, functional and accurate parts using stereolithography machines. The material offers superior chemical resistance and a wid.. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | |
Du-Co Ceramics DC-142 Aluminum Silicate Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | DAM; ISO 178 |
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 24.0 MPa @Strain 3.50 % |
3480 psi @Strain 3.50 % |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® RS LC1610 BK387 Nylon 1010
(Unverified Data**) Plasticized Toughened Renewably Sourced Polyamide 1010 Developed for Extrusion Information provided by DuPont Performance Polymers |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436W10L Wollastonite Reinforced |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436W10L1 Wollastonite Reinforced |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
Ascend Performance Materials Vydyne® 47 BK11 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK11 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
Ascend Performance Materials Vydyne® 47 NT Nylon 66, Impact Modified, Conditioned Vydyne® 47 NT is general-purpose, impact-modified PA66 resin. Available in natural, it is recognized for all the processing and property advantages inherent to PA66 with the addition of improved im.. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
Ascend Performance Materials Vydyne® 47 Nylon 66, Conditioned Vydyne® 47 Nylon resins are general purpose polyamide, impact modified grades. They are available in natural, black and heat stabilized for improved resistance to elevated temperatures. The heat st.. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
Ascend Performance Materials Vydyne® 47H BK0644 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK0644 is a high-performance, medium-impact-modified, heat-stabilized PA66 resin with excellent UV stability and outstanding processing characteristics. This product has an UL746C f1 ra.. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ASTM D790 |
Aclo Accutech Polypropylene Copolymer CP0436C20L1 Calcium Reinforced |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
Ascend Performance Materials Vydyne® 47H BK03 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK03 is a general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
Ascend Performance Materials Vydyne® 47H BK0501 Nylon 66, Impact Modified, Conditioned Vydyne® 47H BK0501 is general-purpose, impact-modified PA66 resin. Available in black, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vyd.. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
Ascend Performance Materials Vydyne® 47H BK0668 Nylon 66, Impact Modified, Heat Stabilized, Conditioned Vydyne® 47H BK0668 is a high-performance, medium-impact-modified, heat-stabilized grade of PA66 resin.Availability:Asia PacificEuropeNorth AmericaAdditive:Impact Modifier Features:Gasoline Resistan.. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
Ascend Performance Materials Vydyne® 47H Nylon 66, Impact Modified, Conditioned Vydyne® 47H is general-purpose, impact-modified PA66 resin. Available in natural, it is heat-stabilized for improved resistance to elevated temperatures. The heat stabilization package for Vydyne 4.. |
|||
Flexural Strength | 24.0 MPa | 3480 psi | ISO 178 |
SABIC Innovative Plastics LNP STAT-KON MS000IL PP LNP* STAT-KON* MS000IL is a compound based on Polypropylene resin containing Stainless Steel. Added features of this material include: High Impact, Low Extractible, Electrically Conductive, food c.. |