Material Notes:
A 2 part solventless and colourless liquid silicone rubber with particularly good adhesion to polyamide as well as glass fabric. Cured rubber coating is high strength and has high elongationInformation provided by Dow Corning
Physical Properties Metric English Comments
Specific Gravity 1.10 g/cc

@Temperature 25.0 °C
1.10 g/cc

@Temperature 77.0 °F
Solids Content <= 98 %
<= 98 %
Viscosity 180000 cP
180000 cP
dynamic
Mechanical Properties Metric English Comments
Hardness, Shore A 30
30
Tensile Strength, Ultimate 7.0002 MPa
1015.3 psi
Elongation at Break 600 %
600 %
Tear Strength 40.06 kN/m
228.5 pli
Processing Properties Metric English Comments
Pot Life 1440 min
1440 min
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Appearance transparent
Mix Ratio (X:1) 100
Base to Catalyst ETN