Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Calcium Carbonate (CaCO3) Filler
Manufacturer Asahi Kasei
Trade Name Thermofil
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei Thermofil P-40CC-1100 40% Calcium Carbonate Reinforced, Heat Stabilized.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Asahi Thermofil
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Linear Mold Shrinkage 0.010 cm/cm
0.010 in/in
ASTM D955
Melt Flow 6.0 g/10 min
6.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 82
82
ASTM D785
Tensile Strength, Yield 22.8 MPa
3300 psi
ASTM D638
Elongation at Yield 55 %
55 %
ASTM D638
Flexural Strength 41.4 MPa
6000 psi
ASTM D790
Flexural Modulus 2.76 GPa
400 ksi
ASTM D790
Izod Impact, Notched 0.320 J/cm
0.600 ft-lb/in
ASTM D256
Izod Impact, Unnotched 8.01 J/cm
15.0 ft-lb/in
ASTM D4812
Thermal Properties Metric English Comments
CTE, linear 50.4 µm/m-°C

@Temperature 20.0 °C
28.0 µin/in-°F

@Temperature 68.0 °F
ASTM D696
Deflection Temperature at 0.46 MPa (66 psi) 121 °C
250 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 76.7 °C
170 °F
ASTM D648
Flammability, UL94 HB
HB
0.0591 in thickness