Mechanical Properties Metric English Comments
Tensile Strength >= 2.07 MPa
>= 300 psi
ASTM D412
Parker Chomerics Tecknit Consil®-R 855 Pure Silver-Filled Silicone Elastomer
Description: CONSIL-RHT 855 is a pure silver-filled silicone elastomer ideal for applications where high temperature is a concernTypical Applications: CONSIL-RHT 855 silicone is used throughout indu..
Tensile Strength 2.07 MPa

@Strain 100 %
300 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R5145B Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 2.07 MPa

@Strain 100 %
300 psi

@Strain 100 %
Type IV, 51 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible 82024 Polyvinyl Chloride, Flexible (PVC, Flexible)
Automotive OEM approval(s).Information provided by PolyOne
Tensile Strength 2.07 MPa

@Strain 100 %
300 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible R5145A Polyvinyl Chloride, Flexible (PVC, Flexible)
Information provided by PolyOne
Tensile Strength 2.07 MPa
300 psi
Measured on solution cast film from toluene; BAM 1245
Kraton® G1642 H (SEBS) Linear Triblock Copolymer
Description: Kraton G1642 H is a clear, linear triblock copolymer based on styrene and ethylene/butylene with a polystyrene content of 20%. It is supplied from North America in the physical form ide..
Tensile Strength 2.07 MPa
300 psi
Typical properties of film cast from toluene solution; ASTM D412
Kraton® G1701 H (SEP) Linear Diblock Copolymer
Description: Kraton G1701 H is a clear, linear diblock copolymer based on styrene and ethylene/propylene with a polystyrene content of 37%. It is supplied from North America in the physical form ide..
Tensile Strength 2.07 MPa
300 psi
Side 2, Silicone Property; ASTM D412
Arlon R36386C035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber (Ferromagnetic Filler) Substrate: Style 7628 Fiberglass This data represents typical value..
Tensile Strength 2.07 MPa
300 psi
Silicone Property; ASTM D412
Arlon Thermabond® R36300W008 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Description: Low Outgassing, Thermally Conductive, Electrically Insulating, Thermabond® Bonds without primerRecommended Primers: Dow Corning S2260Design/Construction: Liner: FEP Product: Uncured S..
Tensile Strength 2.07 MPa
300 psi
Silicone Property; ASTM D412
Arlon Thermabond® R36300W015 0.015" (0.381 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier
Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Primers: Dow Corning S2260Appearance: White silicone gumThis data represents typical val..
Tensile Strength >= 2.07 MPa
>= 300 psi
Compound Property
Arlon R34332X039 0.039" (0.991 mm) Fully Cured/Unsupported
Design/Construction:Overall: Fully cured/unsupported This data Represents typical values for the production material. The data should not be used to write, or in place of, material specifications.In..
Tensile Strength 2.07 MPa
300 psi
ASTM D412
Kraton® G1701 M (SEP) Linear Diblock Copolymer
Description: Kraton G1701 M is a clear, linear diblock copolymer based on styrene and ethylene/propylene with a polystyrene content of 37%. It is supplied from North America in the physical form ide..
Tensile Strength 2.07 MPa
300 psi
Typical properties of film cast from toluene solution; ASTM D412
Kraton® G1702 H (SEP) Linear Diblock Copolymer
Description: Kraton G1702 H is a clear, linear diblock copolymer based on styrene and ethylene/propylene with a polystyrene content of 28%. It is supplied from North America in the physical form ide..