Arlon AD430 Glass, PTFE and Micro-Dispersed Ceramic

Category Polymer , Thermoplastic , Fluoropolymer , PTFE
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon AD430 Glass, PTFE and Micro-Dispersed Ceramic.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High Dielectric Constant for Circuit Militarization & Patch Antenna ApplicationsInformation provided by Arlon Materials for Electronics (MED).
Physical Properties Metric English Comments
Density 2.10 g/cc
0.0759 lb/in³
Water Absorption 0.060 %
0.060 %
Mechanical Properties Metric English Comments
Peel Strength 2.98 kN/m
17.0 pli
Thermal Properties Metric English Comments
CTE, linear 9.00 µm/m-°C
5.00 µin/in-°F
x direction
9.00 µm/m-°C
5.00 µin/in-°F
y direction
CTE, linear, Transverse to Flow 40.0 µm/m-°C
22.2 µin/in-°F
z direction
Thermal Conductivity 0.460 W/m-K
3.19 BTU-in/hr-ft²-°F
Flammability, UL94 V-0
V-0
Electrical Properties Metric English Comments
Dielectric Constant 4.3

@Frequency 1.00e+10 Hz
4.3

@Frequency 1.00e+10 Hz
4.23

@Thickness 3.17 mm
4.23

@Thickness 0.125 in
4.3

@Thickness 0.762 mm
4.3

@Thickness 0.0300 in
Dissipation Factor 0.0030

@Frequency 1.00e+10 Hz
0.0030

@Frequency 1.00e+10 Hz
Descriptive Properties Value Comments
Temperature Coefficient of Dielectric (ppm/°C) -55