Struktol TPW 012 Processing Additive

Category Other Engineering Material , Additive/Filler for Polymer , Polymer
Manufacturer Struktol
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Struktol TPW 012 Processing Additive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
An optimized blend of special waxes and oleo chemicals.STRUKTOL® TPW 012 is a formulated blend of lubricants designed to provide optimum processing, surface and physical property characteristics of rigid PVC compounds. STRUKTOL® TPW 012 is recommended for wood-filled PVC and has been shown to provide significant processing and output rate benefits when compared to traditional lubricant formulations.
Physical Properties Metric English Comments
Specific Gravity 0.980 g/cc
0.980 g/cc
Additive Loading 2.0 - 8.0 %
2.0 - 8.0 %
parts depending on formulation and processing needs.
Thermal Properties Metric English Comments
Dropping Point 122 - 128 °C
252 - 262 °F
Descriptive Properties Value Comments
Appearance Beige to light tan pastilles