Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arlon 55579R055 0.054" (1.37 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 55579R055 0.054" (1.37 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Layer 1, Silicone Property; Arlon SQA-TMS-024
1.35 g/cc
0.0488 lb/in³
Layer 2, Silicone Property; Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Layer 1; Arlon SQA-TMS-003
76.2 microns
3.00 mil
Interleave
457 microns
18.0 mil
Substrate; Arlon SQA-TMS-003
838 microns
33.0 mil
Layer 2; Arlon SQA-TMS-003
1370 microns
54.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 44
44
Layer 1, Silicone Property; ASTM D2240
52
52
Layer 2, Silicone Property; ASTM D2240
Tensile Strength 6.14 MPa
890 psi
Layer 2, Silicone Property; ASTM D412
7.58 MPa
1100 psi
Layer 1, Silicone Property; ASTM D412
Elongation at Break 550 %
550 %
Layer 2, Silicone Property; ASTM D412
650 %
650 %
Layer 1, Silicone Property; ASTM D412
Peel Strength 6.89 kN/m
39.3 pli
Bond Strength; Arlon SQA-TMS-011
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
UL RTI, Electrical 220 °C
428 °F
E54153
UL RTI, Mechanical without Impact 200 °C
392 °F
E54153
Electrical Properties Metric English Comments
Dielectric Strength 25.0 kV/mm
635 kV/in
ASTM D149
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Postcure Cycle
15.0 min

@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour

@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month

@Temperature 21.1 °C
6.00 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Red
Red
Substrate
Total Product Weight (oz/yd2) 51.8
Arlon SQA-TMS-025