Physical Properties Metric English Comments
Thickness 838 - 940 microns
33.0 - 37.0 mil
Side 1
Arlon 10502R030 0.040" (1.02 mm) Cured/Post-Cured Unsupported Silicone Rubber
Design/Construction:Side 1: Cured/Post-Cured Unsupported Silicone Rubber Appearance: Red silicone rubberThis data represents typical values for the production material. The data should not be used t..
Thickness 838 - 940 microns
33.0 - 37.0 mil
Overall
Arlon 51586R035 0.035" (0.889 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mate..
Thickness 838 microns
33.0 mil
Layer 2; Arlon SQA-TMS-003
Arlon 55579R055 0.054" (1.37 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass clot..
Thickness 838 microns
33.0 mil
Layer 2; Arlon SQA-TMS-003
Arlon 55869R062 0.062" Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: 3 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production materia..
Thickness 838 microns
33.0 mil
without liner
3M GM110 Gripping Material
3M™ Gripping Material GM110 is based on 3M’s proprietary micro-replicated technology. 3M griping material GM 110 consists of a high-friction surface with a nylon knit backing that provides stretch..
Thickness 838 microns
33.0 mil
without liner
3M GM400 Gripping Material
3M™ Gripping Material GM400 is based on 3M’s proprietary micro-replicated technology. 3M™ Gripping Material GM110 is based on 3M’s proprietary micro-replicated technology. 3M griping material GM..
Thickness 838 microns
33.0 mil
Interleave 1
Arlon 51991A020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave 2: Polyethylene This data represents typica..
Thickness 838 microns
33.0 mil
layer 2; Arlon SQA-TMS-003
Arlon 55149R062 Silicone Rubber/Fiberglass Laminate
Interleave: 3 mil PE; Layer 2: uncured silicone rubber; Layer 1: cured silicone rubber; Substrate: 162 fiberglass
Thickness 838 microns
33.0 mil
Overall; Arlon SQA-TMS-003
Arlon 55279R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s..
Thickness 838 microns
33.0 mil
Overall; Arlon SQA-TMS-003
Arlon 55589R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass This..
Thickness 838 microns
33.0 mil
ASTM D3752
3M 500 Impact Stripping Tape
3M™ Impact Stripping Tape 500 is a specially compounded light green rubber-backed tape with an acrylic adhesive and easy-release liner. This product can be used for masking and surface protection d..