Arlon 55572GA028 0.028" Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 55572GA028 0.028" Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.24 g/cc
0.0448 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 305 microns
12.0 mil
Side 1; Arlon SQA-TMS-003
406 microns
16.0 mil
Substrate; Arlon SQA-TMS-003
711 microns
28.0 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 44
44
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 7.58 MPa
1100 psi
Silicone Property; Arlon SQA-TMS-008
Elongation at Break 650 %
650 %
Silicone Property; Arlon SQA-TMS-008
Tear Strength 14.5 kN/m
83.0 pli
Die B; Silicone Property; Arlon SQA-TMS-029
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
UL RTI, Electrical 220 °C
428 °F
E54153
UL RTI, Mechanical without Impact 200 °C
392 °F
E54153
Electrical Properties Metric English Comments
Dielectric Strength 18.0 kV/mm
457 kV/in
Arlon SQA-TMS-020
Processing Properties Metric English Comments
Cure Time 120 min

@Temperature 204 °C
2.00 hour

@Temperature 400 °F
Recommended Post Cure Cycle
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Green
Total Product Weight (oz/yd2) 28.1
Arlon SQA-TMS-025