Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 10842S090 Fully Cured, Unsupported Silicone Rubber Product Color: Saddle BrownInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should not be used as material specifications.Information provided by AR.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 27122T125 Cured Silicone Rubber/Skive Tape Laminate Design/Construction:Side 1: Cured Silicone RubberSubstrate: 5.0 mil Etched Skive Tape bonded to one sideThis data represents typical values for the production material and should not be used as ma.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 48146X008 0.0080" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the producti.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 49581R010 0.0105" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1681 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51146R050 0.050" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PEThis data represents typical values for the production materi.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 514B12R006 0.006" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2116 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51576XC15A 0.015" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 2: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 1: Cured Silicone RubberThis data represents typical values for the producti.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51866R015 0.0170" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51866R015E 0.0150" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 55572GA028 0.028" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 55576R060 0.060" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 55578XA028 0.0280" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 2 Layer 2: Uncured Silicone RubberSide 2 Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone RubberThis data represents ty.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 55586XC028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 55986C028 0.0295" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave 1: N/ASide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Uncured Silicone RubberInterleave 2: LDPEThis data represents typical values for the pro.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 56579R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production mate.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 99020N015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction:Interleave: 0.001" FEP FilmSide 1: Uncured Silicone RubberCarrier: 0.003" PTFE coated FiberglassRecommended Primer: Chemlock 607This data represents typical values for the pro.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 99410R015 0.015" Uncured Silicone Rubber with PTFE Coated Fiberglass Substrate Design/Construction:Interleave: 0.001" FEPSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material and sho.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon R30370A008 0.008" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.001" FEP FilmSide 1: Unsupported/Uncured Silicone RubberSubstrate: 0.003" PTFE coated FiberglassThis data represents typical values for the production material a.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon T3020-B004 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate 1.0 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape.Design/Construction:Side 1: Cured Silicone RubberSubstrate: 25% Sinusoidal FiberglassSide 2: Cured Silicone.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 41580B030 0.030" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51103R015 0.0150" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: LDPEThis data represents typical values for the producti.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51163X0085 0.0085" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone Rubber50" wideThis data represents typical values for the production material and should not.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51426W015 0.015" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PolyethyleneThis data represents typical values for the pr.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 51921R020 0.020" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Prime Coated 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon T3020-B002-## 0.020" Self-Fusing, Cured Silicone Rubber Tape with Fiberglass Substrate 0.5 inch wide, 20 mil thick, black, rectangular cross-section, self-fusing silicone tape. Product is supplied in various yard long roll lengths as indicated by the ## characters in the part number... |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 32580R030 0.030" Uncured Silicone Rubber on PET Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberCarrier: 0.005" PETThis data represents typical values for the production material and should not be used as mate.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 41580R025 0.025" Uncured, Unsupported Silicone Rubber on Release Carrier Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured, Unsupported Silicone RubberSubstrate: Holland Cloth CarrierThis data represents typical values for the production material and .. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 44426R010 0.010" Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Cured Silicone RubberSide 2: Uncured Silicone RubberSubstrate: Prime Coated 1165 FiberglassThis data represents typical values for the p.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 47571R012 0.012" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Uncured Silicone RubberSubstrate: Style 2113 FiberglassSide 2: Uncured Silicone RubberInterleave: LDPEThis data represents typical values for the produ.. |
|||
Maximum Service Temperature, Inert | 232 °C | 450 °F | |
Arlon 30850N125 0.125" Uncured, Unsupported Silicone Rubber on a Kodacel Carrier Design/Construction:Side 1: Uncured, Unsupported Silicone RubberSubstrate: Kodacel CarrierInterleave: 0.003" PolyethyleneThis data represents typical values for the production material and should.. |