Processing Properties | Metric | English | Comments |
---|---|---|---|
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning MOLYKOTE® 3452 CHEMICAL RESISTANT VALVE GREASE Fluorosilicone grease thickened with PTFEInformation provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning MOLYKOTE® 44 HIGH TEMPERATURE BEARING GREASE, MEDIUM Phenyl-methyl silicone grease for low to high temperaturesInformation provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning MOLYKOTE® G 68 Semi-synthetic greaseInformation provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning MOLYKOTE® G-00050 FG WHITE EP BEARING GREASE Aluminum complex-thickened mineral oil food grade greaseInformation provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning MOLYKOTE® PG-21 PLASTISLIP GREASE Silicone grease especially for plastic/plastic and plastic/metal combinations like control cables and circuit lever systemInformation provided by Dow Corning |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning XIAMETER® PMCPOHX-4010 Polymer 4000CS Is chemically equivalent to DOW CORNING® 3-0213 POLYMER, 4000CS. Polydimethylsiloxane polymer with terminated, curable silanol functionality, viscosity = 4,000 cp.Information provided by Dow Cornin.. |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning 1-6136 ANTISTAT Dow Corning 1-6136 Antistat is a cationic alkoxy silane and is designated 3-trimethoxysilylpropyloctadecyidimethyl ammonium chloride. It is supplied as a 42 percent active solution (by weight) in me.. |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning 2-0400 DIMETHYLCHLOROSILANE (ME2HSICL) DIST Information provided by Dow Corning |
|||
Shelf Life | 60.0 Month @Temperature 23.0 °C |
60.0 Month @Temperature 73.4 °F |
From date of manufacture |
Arlon 51073R031 0.0311" (0.79 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone Rubber This data represents typical values for the production materi.. |
|||
Shelf Life | 60.0 Month @Temperature 23.0 °C |
60.0 Month @Temperature 73.4 °F |
From date of manufacture |
Arlon 55173R045 0.045" (1.14 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Product Use: Press PadAppearance: Red silicone rubber on f.. |
|||
Shelf Life | 60.0 Month @Temperature 21.1 °C |
60.0 Month @Temperature 70.0 °F |
|
Arlon 55572GA028 0.028" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 162 FiberglassThis data represents typical values for the production material and should not be used as material .. |
|||
Shelf Life | 60.0 Month @Temperature 21.0 - 27.0 °C |
60.0 Month @Temperature 69.8 - 80.6 °F |
From date of manufacture |
Arlon Thermabond® 48A43X008 0.008"(0.203 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® Electrically insulating, thermally conductive, thermal interface material (TIM).Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassSide 2: Cu.. |
|||
Shelf Life | 60.0 Month @Temperature 23.0 °C |
60.0 Month @Temperature 73.4 °F |
From date of manufacture |
Arlon Thermabond® 51A42X012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Thermabond® - Electrically insulating, thermally conductive, thermal interface material (TIM)Design/Construction: Liner: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 7628.. |
|||
Shelf Life | 60.0 Month @Temperature 22.8 °C |
60.0 Month @Temperature 73.0 °F |
|
Arlon UltraPad™ 51073G031D Silicone-Based Press Pad Green UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data.. |
|||
Shelf Life | 60.0 Month @Temperature 22.8 °C |
60.0 Month @Temperature 73.0 °F |
|
Arlon UltraPad™ 51073R031D Silicone-Based Press Pad UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data repre.. |
|||
Shelf Life | 60.0 Month @Temperature 23.0 °C |
60.0 Month @Temperature 73.4 °F |
From date of manufacture |
Arlon Ultrapad™ 55072R125D 0.125" (3.17 mm) Cured Silicone Rubber with Fiberglass Substrate Description: Ultrapad™ Silicone-based press pad. Arlon UltraPad press pad is a high performance, fiberglass reinforced, silicone sheet designed for flex and rigid-flex circuitry lamination. UltraPa.. |
|||
Shelf Life | 60.0 Month @Temperature 22.8 °C |
60.0 Month @Temperature 73.0 °F |
|
Arlon UltraPad™ 55073R031 Silicone-Based Press Pad UltraPad™ D65: Silicone Based Press PadDesign/Construction:Interleave: 3 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberThis data repre.. |
|||
Shelf Life | 60.0 Month @Temperature 21.1 °C |
60.0 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 48362X005 0.005" (0.127 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1080 FiberglassProduct Use: Flexible hose/duct substrateAppearance: Gray silicone rubber on fiberglass fabricThis data represents t.. |
|||
Shelf Life | 60.0 Month @Temperature 23.9 °C |
60.0 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon 510-638R-50 0.008" (0.203 mm) Silicone Rubber Coated Fiberglass 48 inches overall usable width. Design/Construction: Fiberglass fabric primed for adhesion to silicone elastomers vulcanized with organic peroxides.Style: 7628Weave: Plain Count (ends x picks): 44 .. |
|||
Shelf Life | 60.0 Month @Temperature 23.9 °C |
60.0 Month @Temperature 75.0 °F |
|
Arlon 55143R060 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil PE; Side 2: cured silicone rubber; Substrate: 162 fiberglass; Side 1: cured silicone rubber |
|||
Shelf Life | 60.0 Month @Temperature 23.0 °C |
60.0 Month @Temperature 73.4 °F |
From date of manufacture |
Arlon 55173R062 0.0622" (1.58 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Cured Silicone Rubber Substrate: Style 162 Fiberglass Layer 1: Cured Silicone Rubber Product Use: Press PadAppearance: Red silicone rubber on f.. |
|||
Shelf Life | 60.0 Month @Temperature 23.9 °C |
60.0 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon 59463X068CT 0.068" (1.73 mm) Textured, Cured Rubber with Fiberglass Substrate Design/Construction:Side 1: Textured, Cured Rubber Side 2: Textured, Cured Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Shelf Life | 60.0 Month @Temperature 23.9 °C |
60.0 Month @Temperature 75.0 °F |
From date of manufacture |
Arlon 99-108065 PTFE Resin Design/Construction: Side 1: PTFESubstrate: Style 1080 Fiberglass Side 2: PTFE ResinAppearance: Brown Woven FabricThis data represents typical values for the production material. The data should not.. |
|||
Shelf Life | 60.0 Month @Temperature 21.1 °C |
60.0 Month @Temperature 70.0 °F |
From date of manufacture |
Arlon 99202R008 0.008" (0.203 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Carrier Design/Construction: Interleave: FEP FilmSide 1: Cured Silicone Rubber Carrier: PTFE Coated FiberglassProduct Use: Adhesive. Bonds without primer.Appearance: Off-white, High viscosity gum on release.. |
|||
Shelf Life | 60.0 Month @Temperature 21.1 - 26.7 °C |
60.0 Month @Temperature 70.0 - 80.0 °F |
From date of manufacture |
Arlon R35232B085 0.085" (2.16 mm) Fully Cured Silicone Rubber Description: Fully cured, unsupported, static dissipation siliconeDesign/Construction:Liner: Polyethylene Product: Fully Cured Silicone RubberAppearance: Black cured siliconeThis data represents typ.. |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
3M Novec™ Contact Cleaner 3M™ Novec™ Contact Cleaner effectively removes light oils, greases, silicones, dust and particulates from sensitive electrical and electronic equipment. Meets MIL-PRF 29608A Class C specifications.. |
|||
Shelf Life | 60.0 Month | 60.0 Month | |
Dow Corning 3099 HVIC COMPOUND Dow Corning 3099 is a grease-like silicone coating especially formulated to give electrical insulators long-term resistance to water filming and flashover.Features: Protecting electrical insulators... |
|||
Shelf Life | 60.0 Month @Temperature 23.9 °C |
60.0 Month @Temperature 75.0 °F |
|
Arlon R36812T010 0.010" Cured Silicone Rubber with Laminated ETFE Film Substrate Design/Construction:Liner: N/ASide 1: Cured Silicone RubberSubstrate: Laminated ETFE FilmChemical Compatibility: Alkalis, Organic and Inorganic acids, Amines, Epoxies, Aromatic compounds, Chlorin.. |
|||
Shelf Life | 60.0 Month @Temperature 21.0 - 27.0 °C |
60.0 Month @Temperature 69.8 - 80.6 °F |
From date of manufacture |
Arlon R37622X008 0.008" (0.203 mm) Cured Silicone Rubber with Release PET Carrier Description: Thermabond® electrically insulating, thermally conductive, thermal interface materialDesign/Construction: Liner: Polyethylene Product: Cured Silicone Rubber Carrier: PTFE Coated Fiber.. |
|||
Shelf Life | 60.0 Month @Temperature 21.0 - 27.0 °C |
60.0 Month @Temperature 69.8 - 80.6 °F |
From date of manufacture |