Arlon 44562R011 0.011" Cured Silicone Rubber with Fiberglass

Category Polymer , Thermoset , Silicone , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon 44562R011 0.011" Cured Silicone Rubber with Fiberglass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not be used as material specifications.Information provided by ARLON Silicone Technologies Division.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 140 microns
5.50 mil
Silicone; Arlon SQA-TMS-003
140 microns
5.50 mil
Substrate; Arlon SQA-TMS-003
279 microns
11.0 mil
Overall Thickness; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 45
45
Silicone Property; Arlon SQA-TMS-014
Tensile Strength 5.52 MPa
800 psi
Silicone Property; Arlon SQA-TMS-008
Elongation at Break 500 %
500 %
Silicone Property; Arlon SQA-TMS-008
Thermal Properties Metric English Comments
Maximum Service Temperature, Inert 204 °C
400 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Electrical Properties Metric English Comments
Dielectric Strength 29.7 kV/mm
755 kV/in
Arlon SQA-TMS-020
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
Descriptive Properties Value Comments
Color Red
Total Product Weight (oz/yd2) 11
Arlon SQA-TMS-025