Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 279 microns | 11.0 mil | |
Hexcel® HexForce™ 7642 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 280 microns | 11.0 mil | ASTM D374 |
Eastman Eastar A150 Copolyester, Film Eastar A150 Copolyester is a poly(1,4-cyclohexylene-dimethylene terephthalate/isophthalate). It is produced by reacting terephthalic acid and isophthalic acid with the glycol 1,4-cyclohexanedimethan.. |
|||
Thickness | 279 microns | 11.0 mil | Side 1 |
Arlon 51393R031 0.031 (0.635 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Pad Life: 150 Cycles (temperature and time dependent)This data represents typical values for the production material. T.. |
|||
Thickness | 279 microns | 11.0 mil | Nominal |
AK Steel CARLITE® M-4 Grain Oriented Electrical Steel Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce.. |
|||
Thickness | 279 - 330 microns | 11.0 - 13.0 mil | Overall |
Arlon R30082R012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Aluminized PET Film (PET Film/Glass Lamination)Side 2: Cured Silicone Rubber Appearance: Red silicone gum supported on glass fabric with aluminized film backingThis data .. |
|||
Thickness | 279 microns | 11.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon 51808R011 0.011" (0.279 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Wash Coat This data represents typical values for the production .. |
|||
Thickness | 279 microns | 11.0 mil | Layer 2; Arlon SQA-TMS-003 |
Arlon 55589R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass This.. |
|||
Thickness | 279 microns | 11.0 mil | Overall; Arlon SQA-TMS-003 |
Arlon R38095R011 0.011" (0.279 mm) Partially Cross Linked Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Partially Cross Linked Silicone RubberSubstrate: Style 1528 Fiberglass:Side 2: Partially Cross Linked Silicone Rubber Product Use: Electrical InsulationAppearance: Red si.. |
|||
Thickness | 280 microns | 11.0 mil | |
3M Nextel™ AF-12 w/o sizing Aerospace Woven Fabric 312 Information provided by 3M |
|||
Thickness | 280 microns | 11.0 mil | |
3M Nextel™ DF-11 Woven Fabric 610 Information provided by 3M |
|||
Thickness | 279 microns | 11.0 mil | Overall Thickness; Arlon SQA-TMS-003 |
Arlon 44562R011 0.011" Cured Silicone Rubber with Fiberglass Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Thickness | 279 - 330 microns | 11.0 - 13.0 mil | Overall |
Arlon 45541R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or.. |
|||
Thickness | 279 microns | 11.0 mil | Side 1, Uncured Layer; Arlon SQA-TMS-003 |
Arlon R35928R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |
|||
Thickness | 279 - 330 microns | 11.0 - 13.0 mil | Overall |
Arlon 43191R012 0.012" (0.305 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. T.. |