Polymer Property : Thickness = 279 microns Product List

Physical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Physical Properties Metric English Comments
Thickness 279 microns
11.0 mil
Hexcel® HexForce™ 7642 Fiber Glass Fabric
Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential ..
Thickness 279 microns
11.0 mil
Side 1
Arlon 51393R031 0.031 (0.635 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured Silicone Rubber Pad Life: 150 Cycles (temperature and time dependent)This data represents typical values for the production material. T..
Thickness 279 microns
11.0 mil
Nominal
AK Steel CARLITE® M-4 Grain Oriented Electrical Steel
Oriented Electrical Steels are iron-silicon alloys that were developed to provide the low core loss and high permeability required for efficient and economical electrical transformers. First produce..
Thickness 279 - 330 microns
11.0 - 13.0 mil
Overall
Arlon R30082R012 0.012" (0.305 mm) Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Aluminized PET Film (PET Film/Glass Lamination)Side 2: Cured Silicone Rubber Appearance: Red silicone gum supported on glass fabric with aluminized film backingThis data ..
Thickness 279 microns
11.0 mil
Overall; Arlon SQA-TMS-003
Arlon 51808R011 0.011" (0.279 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: Polyethylene Side 2: Uncured Silicone RubberSubstrate: Style 7628 Fiberglass Side 1: Cured Silicone Wash Coat This data represents typical values for the production ..
Thickness 279 microns
11.0 mil
Layer 2; Arlon SQA-TMS-003
Arlon 55589R033 0.033" (0.838 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction: Interleave: PolyethyleneLayer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: 162 Style FiberglassAppearance: Red silicone gum and rubber on fiberglass This..
Thickness 279 microns
11.0 mil
Overall; Arlon SQA-TMS-003
Arlon R38095R011 0.011" (0.279 mm) Partially Cross Linked Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Partially Cross Linked Silicone RubberSubstrate: Style 1528 Fiberglass:Side 2: Partially Cross Linked Silicone Rubber Product Use: Electrical InsulationAppearance: Red si..
Thickness 279 microns
11.0 mil
Overall Thickness; Arlon SQA-TMS-003
Arlon 44562R011 0.011" Cured Silicone Rubber with Fiberglass
Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not be ..
Thickness 279 - 330 microns
11.0 - 13.0 mil
Overall
Arlon 45541R012 0.012" (0.305 mm) Uncured Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured RubberSide 2: Uncured Rubber Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or..
Thickness 279 microns
11.0 mil
Side 1, Uncured Layer; Arlon SQA-TMS-003
Arlon R35928R020 0.020" (0.508 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate
Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: ..
Thickness 279 - 330 microns
11.0 - 13.0 mil
Overall
Arlon 43191R012 0.012" (0.305 mm) Uncured Silicone Rubber with Fiberglass Substrate
Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. T..