Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Strength | 5.52 MPa | 800 psi | |
Teknor Apex Tekbond® TB 2008 Thermoplastic Elastomer Notes: Tekbond® TPEs are a functional series of elastomer compounds designed to not only bond to the most difficult neat and reinforced engineering substrates with no primer or surface treatment, b.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 19562R025 0.025" (0.635 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass clothThis data represents typical values for the production material. The data should not be used to wr.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; Arlon SQA-TMS-008 |
Arlon 19563R032 0.032" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1523 FiberglassSide 2: Cured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the producti.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 30570R010 0.010" (0.254 mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 30570XA015 0.015" (0.381mm) Uncured/Unsupported Silicone Rubber on a Release Carrier Design/Construction:Side 1: Uncured/Unsupported Silicone Rubber on a Release Carrier Appearance: Gray silicone gum on polymer linerThis data represents typical values for the production material. Th.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 31570R025 0.025" (0.635 mm) Uncured Unsupported Silicone on a HDPE Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on a HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The dat.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Compound Property; ASTM D412 |
Arlon 32580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on a PET Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data s.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Compound Property; ASTM D412 |
Arlon 32580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on PET Carrier Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on PET CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data s.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 51629R020 0.020" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil polyLayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassThis data represents typical values for the production mat.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 55900R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: 162 Style Fiberglass Appearance: Red silicone gum on glass fabricThis data represents typical values for the p.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 56596R065 0.065" (1.65 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber Product Use: Flexible heater insulationAppearance: Red silicone gum and rubber on fiberglass with polymer release li.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon CP-301C Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon CP-368 Bulk Compound This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Di.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 32270R060 0.060" (1.52 mm) Uncured Silicone Rubber on PET Carrier Design/Construction: Interleave: PolyethyleneSide 1: Uncured Silicone RubberCarrier: PETAppearance: Red silicone gum on polymer release linerThis data represents typical values for the production ma.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 51103R015 0.0150" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: LDPESide 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Cured Silicone RubberInterleave: LDPEThis data represents typical values for the producti.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 51149R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone RubberSubstrate: Style 7628 FiberglassLayer 1: Cured Silicone RubberThis data represents typical values for the production mat.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 51271R037 0.037" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 2.5 mil PolyethyleneThis data represents typical values for the produ.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 51571R020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Black silicone gum on fiberglass clothThis data Represents typical values for the production material. .. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 51970R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, or .. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 55100R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricT.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Silicone Property; ASTM D412 |
Arlon 55108R030 0.030" (0.762 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Side 2, Layer 2: Uncured Silicone RubberSide 2, Layer 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 1: Cured Silicone Rubber This data rep.. |
|||
Tensile Strength | 5.52 MPa | 800 psi | Layer 2, Silicone Property; ASTM D412 |
Arlon 55279R055 0.055" (1.40 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: Polyethylene Layer 2: Uncured Silicone Rubber Layer 1: Cured Silicone Rubber Substrate: Style 162 Fiberglass Product Use: Flexible heater insulationAppearance: Red s.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 56096R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Silicone Property |
Arlon R31030R025 0.025" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Uncured Silicone RubberSubstrate: 0.015" Prime Coated 1564 FiberglassThis data represents typical values for the production material and.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon R31678R016 0.0175" (0.444 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone/Kapton Side 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass cloth with Kapton® film on opposite side.This data Represents typical va.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon R33089X028 0.029" (0.737 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Cured/Uncured Layers This data Represents typical values for the production material. The data should not be used to write, or in place of, m.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon R33826R017 0.017" (0.432mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon R34369R028 0.029" (0.737 mm) Uncured Layer on Top of a Cured Layer on One Side with Fiberglass Substrate, 38" wide Design/Construction:Side 1: Uncured Layer on Top of a Cured Layer on One SideThis data Represents typical values for the production material. The data should not be used to write, or in place of, ma.. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 44560R009W 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Appearance Red silicone gum on glass fabricThis data represents typical values for the production material. The data should not be used to write, .. |
|||
Tensile Strength | >= 5.52 MPa | >= 800 psi | Compound Property |
Arlon 31580R025 0.025" (0.635 mm) Uncured Unsupported Silicone Rubber on HDPE Carrier
(discontinued **)& Design/Construction:Side 1: Uncured Unsupported Silicone Rubber on HDPE CarrierAppearance: Red silicone gum on polymer linerThis data represents typical values for the production material. The data .. |