Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 140 microns | 5.50 mil | Total |
Parker Chomerics CHO-FAB CRS Shielding Tape Conductive Adhesive Nickel-Plated FabricDescription: CHO-FAB® tape is a corrosion resistant nickel-plated cloth coated with Chomerics’ highly conductive pressure-sensitive adhesive. CHO-FAB® tape.. |
|||
Thickness | 140 microns | 5.50 mil | Liner |
Dielectric Polymers NT-140A89 General Purpose Laminating Adhesive
(discontinued **) Acrylic adhesive with moisture stable PE coated kraft (89#) liner.Features: Plasticizer migration resistantChemical resistantMoisture resistantApplications: Mounting nameplates, signs, graphic panel.. |
|||
Thickness | 140 microns | 5.50 mil | |
Hexcel® HexForce™ 3731 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 140 microns | 5.50 mil | |
Hexcel® HexForce™ 1557 Fiber Glass Fabric Fiber glass in fabric form offers an excellent combination of properties from high strength to fire resistance. Wide ranges of yarn sizes and weave patterns provide huge number of design potential .. |
|||
Thickness | 140 microns | 5.50 mil | Total |
3M 2191FR EMI Shielding Tape 3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by.. |
|||
Thickness | 140 microns | 5.50 mil | Caliper; ASTM D645 |
3M 6142 Medium Duty Water Activated Paper Tape 3M™ Medium Duty Water Activated Paper Tape 6142 is used for box sealing and other packaging applications. This product has a paper backing and a gummed, high tack, water-activated, modified cornsta.. |
|||
Thickness | 140 microns | 5.50 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 49442R0075 0.0075" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 1681 FiberglassThis data represents typical values for the production material and should not be used as material specifications.I.. |
|||
Thickness | 140 microns | 5.50 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 49442R0075EP 0.0075" (0.190 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Substrate: Style 1681 FiberglassSide 2: Acrylic PSAThis data Represents typical values for the production material. The data should not be used to w.. |
|||
Thickness | 140 microns | 5.50 mil | Prime Coated 1681 Fiberglass, Substrate |
Arlon 49576R015 0.015" (0.381 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data Represents typical values for the production mat.. |
|||
Thickness | 140 microns | 5.50 mil | Substrate |
Arlon 49581R010 0.0105" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 3 mil PolyethyleneSide 1: Uncured Silicone RubberSubstrate: Prime Coated 1681 FiberglassSide 2: Uncured Silicone RubberThis data represents typical values for the .. |
|||
Thickness | 140 microns | 5.50 mil | Prime Coated 1681 Fiberglass, Substrate |
Arlon 49581R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The.. |
|||
Thickness | 140 microns | 5.50 mil | side 2 silicone; Arlon SQA-TMS-003 |
Arlon 51106R015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 140 microns | 5.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51866R015 0.0170" Cured/Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 7628 FiberglassSide 2: Uncured Silicone RubberInterleave: 3 mil PEThis data represents typical values for the production material .. |
|||
Thickness | 140 microns | 5.50 mil | Layer 1; Arlon SQA-TMS-003 |
Arlon 56579R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production mate.. |
|||
Thickness | 140 microns | 5.50 mil | Aluminum |
3M 434 Vibration Damping Tape 3M™ Vibration Damping Tapes are low temperature 3M™ Viscoelastic Damping Polymers Tape 830 coated on the dead soft aluminum foil constraining layer. They have pressure sensitive properties and are.. |
|||
Thickness | 140 microns | 5.50 mil | Prime Coated 1165 Fiberglass, Substrate |
Arlon 44571R008A 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 140 microns | 5.50 mil | Prime Coated 1681 Fiberglass, Substrate |
Arlon 49581XC010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Gray gum on glass fiber fabricThis data Represents typical values for the production material. The data .. |
|||
Thickness | 140 microns | 5.50 mil | side 2 silicone; Arlon SQA-TMS-003 |
Arlon 51146R015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 140 microns | 5.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51576W015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: 7628 Style Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: White silicone gum on glass fabricThis data re.. |
|||
Thickness | 140 - 216 microns | 5.50 - 8.50 mil | Side 1 |
Arlon 51970R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, or .. |
|||
Thickness | 140 microns | 5.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51986XA015 0.016" (0.406 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Appearance: Gray silicone gum and rubber on fiberglass clo.. |
|||
Thickness | 140 microns | 5.50 mil | Substrate; Arlon SQA-TMS-003 |
Arlon R38020B020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material. The data should not be used to wr.. |
|||
Thickness | 140 - 165 microns | 5.50 - 6.50 mil | Film and adhesive |
3M 3635-100 Light Enhancement Film A light box or channel letter contains lighting elements that illuminate the front sign face and transmit some light to the viewer. However much of the illumination is reflected or absorbed by other.. |
|||
Thickness | 140 microns | 5.50 mil | Tape |
3M 469 Splicing Tapes 3M™ Splicing Tapes utilize on acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Thickness | 140 microns | 5.50 mil | Total Thickness |
3M 9731RW Double Coated Tape 3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other .. |
|||
Thickness | 140 microns | 5.50 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 44562R011 0.011" Cured Silicone Rubber with Fiberglass Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Thickness | 140 microns | 5.50 mil | Overall; Arlon SQA-TMS-003 |
Arlon 43362X0055 0.0055" (0.140 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2112 FiberglassFlame Resistance: Product meets Title 14 CFR 25.856(a) Appendix F, Part VI (amdt. 25-111) fl.. |
|||
Thickness | 140 microns | 5.50 mil | Overall Thickness |
Arlon 48576R006 0.0055" Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 0.0015" PolyethyleneSide 1: Uncured RubberSubstrate: Prime Coated 1080 FiberglassSide 2: Uncured RubberThis data represents typical values for the production mater.. |
|||
Thickness | 140 microns | 5.50 mil | Overall thickness; Arlon SQA-TMS-003 |
Arlon R37582R0055 0.0055" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Thickness | 140 microns | 5.50 mil | Overall thickness; Arlon SQA-TMS-003 |
Arlon R3758R0055 0.065" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassThis data represents typical values for the production material and should not be .. |