Physical Properties | Metric | English | Comments |
---|---|---|---|
Thickness | 140 microns | 5.50 mil | Typical; TAPPI-411 |
DuPont™ Nomex® 411 Paper, 5 mil Nominal Thickness Nomex® Type 411 is the uncalendared precursor of Type 410. It has a lower density and lower property values. It is used in applications such as motor phase insulation and transformer coil end fil.. |
|||
Thickness | 140 microns | 5.50 mil | Total |
3M 2191FR EMI Shielding Tape 3M EMI Shielding Tapes are well suited for applications requiring reliable point-to-point electrical contact, particularly EMI shielding, grounding and static charge draining.Information provided by.. |
|||
Thickness | 140 microns | 5.50 mil | Caliper |
3M 3028EK Double Coated Tapes with Adhesive 350 3M™ Double Coated Tapes 9500PC, 9500B, 9593 and 3028EK feature a thin polyester film for dimensional stability and improved handling with ease of die-cutting and laminating. 3M™ Adhesive 350 is a .. |
|||
Thickness | 140 - 216 microns | 5.50 - 8.50 mil | Side 2 |
Arlon 19566R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum on fiberglass fabricThis data represents typical values for the production material. The.. |
|||
Thickness | 140 - 216 microns | 5.50 - 8.50 mil | Side 2 |
Arlon 19576R025 0.025" (0.635 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSide 2: Uncured Silicone Rubber Appearance: Red silicone gum and rubber on fiberglass clothThis data represents typical values for the production mat.. |
|||
Thickness | 140 microns | 5.50 mil | Style 1681 Fiberglass, Substrate; Arlon SQA-TMS-003 |
Arlon 49481R030 0.030" (0.762 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave 1: Polyethylene Side 1: Uncured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave 2: Polyethylene This data represents typical .. |
|||
Thickness | 140 microns | 5.50 mil | Prime Coated 1681 Fiberglass, Substrate |
Arlon 49581R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Red silicone gum on fiberglass clothThis data Represents typical values for the production material. The.. |
|||
Thickness | 140 microns | 5.50 mil | Prime Coated 1681 Fiberglass, Substrate |
Arlon 49581X010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberThis data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 140 microns | 5.50 mil | Side 2; Arlon SQA-TMS-003 |
Arlon 51986R015 0.0165" (0.419 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 7628 Fiberglass Side 2: Uncured Silicone Rubber Interleave: Polyethylene Product Use: Flexible heater substrateAppearance: Red colo.. |
|||
Thickness | 140 microns | 5.50 mil | Layer 1; Arlon SQA-TMS-003 |
Arlon 56579R028 0.0295" Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 2.5 mil PELayer 2: Uncured Silicone RubberLayer 1: Cured Silicone RubberSubstrate: Style 1564 FiberglassThis data represents typical values for the production mate.. |
|||
Thickness | 140 microns | 5.50 mil | side 2; Arlon SQA-TMS-003 |
Arlon I51576R015 Silicone Rubber/Fiberglass/Alloy Laminate Top layer of side 2: alloy 600 foil; Bottom layer of side 2: cured silicone rubber; Substrate is 7628 fiberglass; Side 1: cured silicone rubber |
|||
Thickness | 140 microns | 5.50 mil | ASTM D3652 |
3M Scotch® 892 Filament Tape Scotch® Tape 892 is a glass filament reinforced tape suitable for most strapping, bundling, and reinforcing applications. The tape has a synthetic rubber resin adhesive with good shear strength to .. |
|||
Thickness | 140 microns | 5.50 mil | Prime Coated 1165 Fiberglass, Substrate |
Arlon 44571R008A 0.0085" (0.216 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone Rubber Side 2: Uncured Silicone RubberThis data represents typical values for the production material. The data should not be used to write, or in place .. |
|||
Thickness | 140 microns | 5.50 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 49100R010 0.010" (0.254 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: PolyethyleneSide 1: Uncured Silicone Rubber Substrate: Style 1681 FiberglassProduct Use: Flexible heater insulationAppearance: Red silicone gum on fiberglass fabricTh.. |
|||
Thickness | 140 microns | 5.50 mil | substrate; Arlon SQA-TMS-003 |
Arlon 49283R040 Silicone Rubber/Fiberglass Laminate Interleave: 3 mil polyethylene; Side 1: cured silicone rubber; Substrate: 1681 Fiberglass; Side 2: cured silicone rubber |
|||
Thickness | 140 microns | 5.50 mil | Prime Coated 1681 Fiberglass, Substrate |
Arlon 49581XC010 0.0105" (0.267 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberSide 2: Uncured Silicone RubberAppearance: Gray gum on glass fiber fabricThis data Represents typical values for the production material. The data .. |
|||
Thickness | 140 microns | 5.50 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 49586B010 0.0115" (0.292 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction: Side 1: Cured Silicone RubberSubstrate: Style 1681 FiberglassSide 2: Uncured Silicone RubberInterleave: Polyethylene This data represents typical values for the production mater.. |
|||
Thickness | 140 microns | 5.50 mil | side 2 silicone; Arlon SQA-TMS-003 |
Arlon 51146R015 Silicone Rubber/Fiberglass Laminate Side 1: cured silicone rubber; Substrate: 7628 fiberglass; Side 2: uncured silicone rubber; Interleave: 3 mil polyethylene |
|||
Thickness | 140 - 216 microns | 5.50 - 8.50 mil | Side 1 |
Arlon 51970R015 0.015" (0.381 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Uncured Silicone RubberAppearance: Red gum on glass fiber fabricThis data Represents typical values for the production material. The data should not be used to write, or .. |
|||
Thickness | 140 microns | 5.50 mil | Prime Coated 1165 Fiberglass, Substrate |
Arlon R33826R017 0.017" (0.432mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone Rubber Side 2: Uncured Silicone Rubber This data Represents typical values for the production material. The data should not be used to write, or in place o.. |
|||
Thickness | 140 microns | 5.50 mil | Substrate; Arlon SQA-TMS-003 |
Arlon R38020B020 0.020" (0.508 mm) Uncured Silicone Rubber with Fiberglass Substrate Design/Construction: Interleave: LDPESide 1: Uncured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material. The data should not be used to wr.. |
|||
Thickness | 140 - 165 microns | 5.50 - 6.50 mil | Film and adhesive |
3M 3635-100 Light Enhancement Film A light box or channel letter contains lighting elements that illuminate the front sign face and transmit some light to the viewer. However much of the illumination is reflected or absorbed by other.. |
|||
Thickness | 140 microns | 5.50 mil | Tape |
3M 469 Splicing Tapes 3M™ Splicing Tapes utilize on acrylic pressure sensitive adhesive system that offers a balance of initial adhesion and good holding power.Information provided by 3M |
|||
Thickness | 140 microns | 5.50 mil | Total Thickness |
3M 9731RW Double Coated Tape 3M™ Double Coated Tapes 9731 and 9731RW have a firm, silicone pressure sensitive adhesive coated on one side of a polyester film carrier and a high performance acrylic adhesive coated on the other .. |
|||
Thickness | 140 microns | 5.50 mil | Substrate |
Arlon 44426R010 0.010" Cured/Uncured Silicone Rubber Laminate with Fiberglass Substrate Design/Construction:Interleave: 0.003" PolyethyleneSide 1: Cured Silicone RubberSide 2: Uncured Silicone RubberSubstrate: Prime Coated 1165 FiberglassThis data represents typical values for the p.. |
|||
Thickness | 140 microns | 5.50 mil | Substrate; Arlon SQA-TMS-003 |
Arlon 44562R011 0.011" Cured Silicone Rubber with Fiberglass Design/Construction:Interleave: 2.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 1165 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Thickness | 140 microns | 5.50 mil | Overall; Arlon SQA-TMS-003 |
Arlon 440-638RF 0.0055" (0.140 mm) Style 1165 Plain Weave, Prime Coated Fiberglass Design/Construction:Fiberglass Fabric primed for adhesion to silicone elastomers vulcanized with organic peroxides.Material: Prime Coated FiberglassCount: 60x52 (Ends x Picks)This data represents ty.. |
|||
Thickness | 140 microns | 5.50 mil | Overall thickness; Arlon SQA-TMS-003 |
Arlon R37582R0055 0.0055" Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: 1.5 mil PolyethyleneSide 1: Cured Silicone RubberSubstrate: Style 2113 FiberglassThis data represents typical values for the production material and should not be .. |
|||
Thickness | 140 microns | 5.50 mil | Overall; Arlon SQA-TMS-003 |
Arlon R37652R0055 0.0055" (0.140 mm) Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Side 1: Cured Silicone RubberSubstrate: Style 2113 Fiberglass Appearance: Red silicone rubber on fiberglass clothThis data Represents typical values for the production material. .. |