Material Notes:
Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.11 g/cc
0.0401 lb/in³
Arlon SQA-TMS-024
Thickness 76.2 microns
3.00 mil
Polyethylene Interleave
457 microns
18.0 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
Compound Property; ASTM D2240
Tensile Strength 8.62 MPa
1250 psi
Compound Property; ASTM D412
Tensile Strength, Yield 1.72 MPa

@Strain 100 %
250 psi

@Strain 100 %
Compound Property; Arlon SQA-TMS-008
Elongation at Break 800 %
800 %
Compound Property; ASTM D412
Tear Strength >= 38.6 kN/m
>= 220 pli
Compound Property; ASTM D624
Compression Set 19 %
19 %
Compound Property; Arlon SQA-TMS-017
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 232 °C
450 °F
Minimum Service Temperature, Air -56.7 °C
-70.0 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 21.1 °C
60.0 Month

@Temperature 70.0 °F
From date of manufacture
Descriptive Properties Value Comments
Color Saddle Brown
Total Product Weight (oz/yd2) 15.1
Arlon SQA-TMS-025