Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tear Strength | 38.6 kN/m | 220 pli | ASTM D624 |
Multibase Multi-Flex® A 7727 E Black TPE Thermoplastic Elastomer Forms: PelletsProcessing Methods:Injection Molding Information provided by Multibase |
|||
Tear Strength | 38.6 kN/m | 220 pli | Die C |
Taiwan PU Corporation UR60 Polyester Urethane Rubber UR60 is a polyester urethane rubber which is an easy to process millable gum especially developed for improved compounding and processing benefits. It can be processed and compounded by the use of .. |
|||
Tear Strength | 38.6 kN/m | 220 pli | ASTM D624 |
STAR Thermoplastic Alloys & Rubbers StarFlex® P 7390-9000 TPE Product Description: StarFlex P 7390-9000 is an easy processing TPE designed for injection molding Features:Soft TouchRubbery FeelGood WeatherabilityFDA and medical grades availableProcessing Method.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | Die B, 20 in/min; ASTM D624 |
Teknor Apex Monprene® MP-1500 Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | Die B |
Shin-Etsu Silicones KE-5540U Low Temperature Silicone Elastomer ShinEtsu KE5540 U is a nominal 40 Durometer phenyl (PVMQ) base.Product Features: This material was designed for its excellent vibration dampening characteristics. Because of its phenyl content, it a.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | ASTM D624 |
Teknor Apex Monprene® MP-3955B Thermoplastic Elastomer Uses: Closures; Consumer Applications; Gaskets; Handles; Kitchenware; Medical/Healthcare Applications; Packaging; Safety Equipment; Sporting Goods; Toothbrush Handles; Tubing; Writing Instruments Fo.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 30 PHR Fumed Silica - Wacker HK N20 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | |
Dow Corning C6-180 ELASTOMER KIT Two-part, platinum-catalyzed (1:1 by weight), silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices, and fabricating extruded.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | |
Dow Corning C6-350LH ELASTOMER KIT Two-part, platinum-catalyzed (1:1 by weight), silicone elastomers are heat cured high consistency silicone rubbers designed for use by customers fabricating medical devices, and fabricating extruded.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | |
Dow Corning SILASTIC® LS 5-2040 FLUOROSILICONE RUBBER 40 Durometer, off-white, molding grade fluorosilicone base.Information provided by Dow Corning |
|||
Tear Strength | 38.6 kN/m | 220 pli | |
Dow Corning SILASTIC® Q7-4565 BIOMEDICAL GRADE ETR ELASTOMER One-part, enhanced tear-resistant silicone elastomers; uncatalyzed (customer selects peroxide catalyst) elastomer materials designed for compounding into elastomer for part fabrication and medical d.. |
|||
Tear Strength | >= 38.6 kN/m | >= 220 pli | Compound Property; ASTM D624 |
Arlon 10842S018 0.018" (0.457 mm) Fully Cured, Unsupported, Silicone Rubber Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | Die B, Silicone Property; ASTM D624 |
Arlon R37292S018 0.018" (0.457 mm) Cured Silicone Rubber with PTFE Coated Fiberglass Substrate Design/Construction: Interleave: PolyethyleneSide 1: Cured Silicone RubberCarrier: PTFE Coated FiberglassThis data represents typical values for the production material. The data should not be used .. |
|||
Tear Strength | 38.6 kN/m | 220 pli | ISO 34-1 |
Alliance Polymers Viprene™ G70A-32U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | ISO 34-1 |
Alliance Polymers Viprene™ G70A-32U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ G70A-32U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | ISO 34-1 |
Alliance Polymers Viprene™ P60A-22U-BLK Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-BLK is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | ISO 34-1 |
Alliance Polymers Viprene™ P60A-22U-NAT Thermoplastic Vulcanizate Elastomer Viprene™ P60A-22U-NAT is a UV and Heat Stabilized TVP (Thermoplastic Vulcanizate Elastomer). This material can be easily processed by extrusion or injection molding. It exhibits easy flowing charac.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | Die C (graves), 20 in/min; ASTM D624 |
PolyOne Synprene® RT-3870MS Thermoplastic Elastomer - SBC
(discontinued **) Description/Features:High Performance Thermoplastic ElastomerUV StabilizedTranslucentApplications:Multi-PurposeMarket:Consumer GoodsProcessing Method:Injection MoldingPolyOne First ChoiceInformation.. |
|||
Tear Strength | 38.6 kN/m | 220 pli | Die C |
TSE Industries Millathane® E34 Millable Polyether Polyurethane Rubber with 30 PHR Fumed Silica - Wacker HK N20 MILLATHANE E34 is a high performance polyether polyurethane rubber for applications requiring: high abrasion resistance, low temperature flexibility, ozone resistance, oil and fuel resistance, outst.. |