Mechanical Properties Metric English Comments
Tensile Strength, Yield 1.72 MPa

@Temperature 25.0 °C
250 psi

@Temperature 77.0 °F
Lord Adhesives Circalokâ„¢ 6715 Silicone Encapsulant
Circalokâ„¢ 6715 is a two component, medium viscosity, solvent-free silicone which cures at room temperature to an elastomeric, stress-free rubber of outstanding electrical and high temperature p..
Tensile Strength, Yield 1.72 MPa
250 psi
Elastic; ASTM D412
Multibase Multi-Flex® A 0740 TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Colorability, GoodElasticity, HighElectrically InsulatingFlame RetardantFlexibility, GoodHardness, LowHeat StabilizedOzone ResistantProcessability, GoodSoftUV R..
Tensile Strength, Yield 1.72 MPa
250 psi
at 100% secant; ASTM D638
Multibase Multi-Flex® A 5904 LC TPE Thermoplastic Elastomer
Features: Chemical Resistance, Good Heat StabilizedOzone Resistant Forms:PelletsProcessing Method:Injection Molding Information provided by Multibase
Tensile Strength, Yield 1.72 MPa
250 psi
ASTM D-412 (Die C)
Saint-Gobain Norcrylâ„¢ A2000 Solid Acrylic Bonding Tape
Description: The Norcrylâ„¢ solid acrylic core has outstanding internal strength. Norcrylâ„¢ structural grade bonding power can reduce or replace conventional fasteners, rivets, liquid adhesiv..
Tensile Strength, Yield 1.72 MPa

@Strain 300 %
250 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP 1871R Thermoplastic Elastomer
Notes: USP Class VI; ISO 10993; Clear Features: Good Stability Uses: Medical TubingInformation Provided by Teknor Apex
Tensile Strength, Yield 1.72 MPa

@Strain 300 %
250 psi

@Strain 300 %
ASTM D412
Teknor Apex Monprene® MP 1257 Thermoplastic Elastomer
Notes: General Purpose; CSA Approved; OpaqueInformation Provided by Teknor Apex
Tensile Strength, Yield 1.72 MPa
250 psi
Master Bond Mastersil 800 One Component, Room Temperature Curing Silicone
MasterSil 800 is an easy to use, one component, high performance silicone elastomer compound for bonding, sealing, coating and formed-in-place gaskets. This specialty system features ultra high temp..
Tensile Strength, Yield 1.72 MPa

@Strain 100 %
250 psi

@Strain 100 %
Compound Property; Arlon SQA-TMS-008
Arlon 10842S018 0.018" (0.457 mm) Fully Cured, Unsupported, Silicone Rubber
Design/Construction:Side 1: Fully Cured, Unsupported, Silicone Rubber Appearance: Dark red silicone rubberThis data represents typical values for the production material. The data should not be used..
Tensile Strength, Yield 1.72 MPa
250 psi
100%; ASTM D412
Teknor Apex APEX® 3050-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-Natural Color, OpaqueForms-PelletsProcessin..
Tensile Strength, Yield 1.72 MPa
250 psi
TM R050-36
Resinlab® EP1200LV Casting Resin
Resinlab™ EP1200LV a low viscosity version of EP1200, a highly filled, medium viscosity black casting resin designed for applications requiring a high degree of thermal conductivity, flexibility an..
Tensile Strength, Yield 1.72 MPa
250 psi
at 100%
Resinlab® UR3010 Black Polyurethane Potting System
Resinlab™ UR 3010 Black is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro..
Tensile Strength, Yield 1.72 MPa
250 psi
at 100%
Resinlab® UR3010 Clear Polyurethane Potting System
Resinlab™ UR 3010 Clear is a, two component, room temperature curing polyurethane potting system. It is designed to cure completely at room temperature. UR 3010 provides excellent environmental pro..
Tensile Strength, Yield 1.72 MPa
250 psi
at 100%; ASTM D412
G-2712 Styrene-based Biomedical Elastomer
Tensile Strength, Yield >= 1.72 MPa
>= 250 psi
No units listed, assumed to be psi.
Cos40 Cork/Neoprene Rubber Sheet
Description: Harvested every 9-12 years from the cork oak tree, cork is able to rebound from compression with extrusion. Applications include: stoppers, soundproofing, flooring, gaskets, and many ot..
Tensile Strength, Yield 1.72 MPa
250 psi
Transverse/Width
Saint-Gobain Norton® Fluorglas® Chemfilm® R128/R129 Premium Grade Extruded Full Density PTFE Film (0.002" thick)