Material Notes:
Designation ISO 1874-PA11,EHLS,18-010,CD10Grade with graphite filler for tubes extrusion. Available color: steel gray. Light and heat stabilized.No need of lubricant. Low friction coefficient. Good abrasion resistance. High chemical resistance.Example applications: Control cable tubing.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Water Absorption 1.7 %
1.7 %
Melt Flow 1.0 g/10 min

@Load 2.16 kg,
Temperature 235 °C
1.0 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 48.0 MPa
6960 psi
50 mm/min
Elongation at Break 27 %
27 %
Nominal Strain; 50 mm/min
Elongation at Yield 5.0 %
5.0 %
50 mm/min
Tensile Modulus 2.23 GPa
323 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
14.2 J/cm²

@Temperature -30.0 °C
67.6 ft-lb/in²

@Temperature -22.0 °F
Charpy Impact, Notched 0.450 J/cm²
2.14 ft-lb/in²
0.420 J/cm²

@Temperature -30.0 °C
2.00 ft-lb/in²

@Temperature -22.0 °F
Thermal Properties Metric English Comments
Melting Point 183 °C
361 °F
10°C/min
Flammability, UL94 V-2

@Thickness 1.60 mm
V-2

@Thickness 0.0630 in
V-2

@Thickness 3.20 mm
V-2

@Thickness 0.126 in