Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Cycoloy® FXC810AL PC+ABS (Europe-Africa-Middle East) CYCOLOY FXC810AL is a multi-purpose PC+ABS injection moulding grade, suitable for those applications that require Alpine White colour effects. The colour package may effect performance.This data was.. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HPF1 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer Healthcare Grade |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® LUX1832 PC MFR=3.0; Branched extrusion grade for LED applications, UV stabilized; available in diffuse colors |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® LUX9610 PC (Asia Pacific) Lexan LUX9610 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS require.. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® LUX9610 PC (Europe-Africa-Middle East) Lexan LUX9610 is a UV stabilized flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance providing good colorstab.. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® LUX9612G PC (Asia Pacific) Lexan LUX9612G is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS require.. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® LUX9612G PC (Europe-Africa-Middle East) Lexan LUX9612G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® LUX9616G PC (Asia Pacific) Lexan LUX9616G is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requirem.. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® 9925A PC (Asia Pacific) Lexan 9925A is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® EXRL2032 PC (Asia Pacific) Lexan EXRL2032 is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR performance. It intended to meet WEEE/RoHS requir.. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® FXE9925A PC (Asia Pacific) Illuminate / edge glow color effect grade of Lexan 9925A. 9925A is a flame retardant transparent polycarbonate featuring non brominated and non chlorinated FR system with good flow and thin wall FR .. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® LUX9612 PC (Asia Pacific) Lexan LUX9612 is a flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effective and thin wall FR performance. It intended to meet WEEE/RoHS requireme.. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics Lexan® LUX9616G PC (Europe-Africa-Middle East) Lexan LUX9616G (EXRL0945) is a UV stabilized high viscosity, flame retardant polycarbonate featuring non brominated and non chlorinated FR system with diffusion effect and thin wall FR performance p.. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min; ISO 527 |
LG Chemical XR-472 ABS, High Heat Resistance, High Gloss Information Provided by LG Chem |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | |
Henkel Hysol EA 9309.3NA Paste Adhesive System Toughened adhesive with excellent peel strength. Contains glass beads for bond line control.Applications: Structural Repair Composite Bonding |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing 15% PTFE/Silicone. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DP003 PC (Asia Pacific) LNP LUBRICOMP* DP003 is a compound based on Polycarbonate resin containing Silicone, PTFE. Added features of this material include: Internally Lubricated. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP DX09407H PC LNP* LUBRICOMP* DX09407H is a compound based on High Heat Polycarbonate containing proprietary fillers. Added features of this grade are: Wear Resistant, Healthcare. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 50 mm/min; ASTM D638 |
SABIC Innovative Plastics LNP LUBRICOMP QP004 PA 6/10 LNP* LUBRICOMP* QP004 is a compound based on Nylon 6/10 containing 20% PTFE/Silicone. Added feature of this grade is: Wear Resistant. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 50 mm/min; ASTM D 638 |
SABIC Innovative Plastics Xenoy® X6125 PBT+PC Unreinforced, impact modified, thermoplastic alloy (PBT+PC). High impact strength while retaining mechanical and thermal properties.This data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min; ISO 527 |
SABIC Innovative Plastics LNP STAT-KON RD000IXP PA 66 LNP STAT-KON* RD000IXP is a compound based on Nylon 66 resin containing Carbon Powder. Added features of this material include: Electrically Conductive, High Impact. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | ISO 527; DIN 53452 |
Zell-Metall Engineering Plastics Zellamid 1400T (PET + solid lubricant) Zellamid® 1400 is the registered trademark of Zell-Metalls partly crystalline thermoplastic Polyester based on Polyethylene Terephthalate.This PETP features outstanding dimensional stability, .. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 1 mm/min |
Arkema Group Cristamid® MS 1300 Semi-Aromatic Nylon (PASA) (Dry) Designation ISO 1874-PA12/xx,MR,12-020Semi-aromatic polyamide (PASA) grade for injection molding and tubes extrusion.Transparency even thick. High resistance to environmental stress cracking. Good t.. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 5 mm/min; ASTM D 638 |
SABIC Innovative Plastics Lexan® EXRL0681 PC Copolymer 25 MFR LEXAN High Flow Ductile CopolymerThis data was supplied by SABIC-IP for the Americas region. |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized, available in transparent colors only |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Asia Pacific) 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1711 PC Copolymer (Europe-Africa-Middle East) 25 MFR LEXAN High Flow Ductile Copolymer |
|||
Tensile Modulus | 2.23 GPa | 323 ksi | 5 mm/min; ASTM D638 |
SABIC Innovative Plastics Lexan® HFD1731 PC Copolymer (Europe-Africa-Middle East) 25 MFR LEXAN High Flow Ductile Copolymer UV-stabilized |