Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Conditioned)

Category Polymer , Thermoplastic , Elastomer, TPE , Polyether Block Amide (PEBA)
Manufacturer Arkema
Trade Name Pebax®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
Material Notes:
POLYETHER BLOCK AMIDE (PEBA) Supersoft grade (hardness 72 shore A) Modified 2533SN01 Applications: sport (tennis shoes parts)ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 0.960 g/cc
0.0347 lb/in³
Melt Flow 14 g/10 min

@Load 1.00 kg,
Temperature 235 °C
14 g/10 min

@Load 2.20 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Hardness, Shore A 72
72
Tensile Strength, Yield 1.80 MPa

@Strain 50.0 %
261 psi

@Strain 50.0 %
50 mm/min
Tensile Modulus 0.00400 GPa
0.580 ksi
1 mm/min
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 200 µm/m-°C

@Temperature 20.0 °C
111 µin/in-°F

@Temperature 68.0 °F
Melting Point 135 °C
275 °F
(Dry)
Vicat Softening Point 59.0 °C
138 °F
50°C/hr; 50N
Electrical Properties Metric English Comments
Surface Resistance 3.00e+12 ohm
3.00e+12 ohm