Electrical Properties | Metric | English | Comments |
---|---|---|---|
Surface Resistance | 3.00e+12 ohm | 3.00e+12 ohm | ASTM D257 |
Rogers Corporation Poron® 4701-60-15 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Surface Resistance | 3.00e+12 ohm | 3.00e+12 ohm | ASTM D257 |
Rogers Corporation Poron® 4701-60-20 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability tests UL HBF (File E20305), MVSS 302, and CSA Component Acceptance HBF (File 188149). Passes fogging test SAE-J 1736 for 3 h.. |
|||
Surface Resistance | 3.00e+12 ohm | 3.00e+12 ohm | ASTM D257 |
Rogers Corporation Poron® 4701-60-30 Cellular Urethane Foam Standard color is black (04); others are available. Passes flammability test MVSS 302. Passes fogging test SAE-J 1736 for 3 hrs. at 100°C (212°F). Passes cold flexibility per MIL-P-12420D at -4.. |
|||
Surface Resistance | 3.00e+12 ohm @Temperature 23.0 °C |
3.00e+12 ohm @Temperature 73.4 °F |
ASTM D257 |
DuPont Performance Polymers Crastin® 6130 NC010 PBT
(Unverified Data**) Crastin® 6130 NC010 is an unreinforced, medium high viscosity polybutylene terephthalate resin for extrusion and injection molding.Information provided by DuPont Performance Polymers |
|||
Surface Resistance | 3.00e+12 ohm @Temperature 20.0 °C |
3.00e+12 ohm @Temperature 68.0 °F |
65% RH; ASTM D257 |
Arkema Group Pebax® 2533 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Surface Resistance | 3.00e+12 ohm | 3.00e+12 ohm | |
Arkema Group Pebax® 2533 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 25 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Surface Resistance | 3.00e+12 ohm | 3.00e+12 ohm | |
Arkema Group Pebax® 3533 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 35 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Surface Resistance | 3.00e+12 ohm | 3.00e+12 ohm | |
Arkema Group Pebax® 4033 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) hardness 40 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: molded parts for sport goods (softness.. |
|||
Surface Resistance | 3.00e+12 ohm @Temperature 20.0 °C |
3.00e+12 ohm @Temperature 68.0 °F |
65% RH; ASTM D257 |
Arkema Group Pebax® 5533 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
Surface Resistance | 3.00e+12 ohm | 3.00e+12 ohm | |
Arkema Group Pebax® MX 1283 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE (PEBA) Supersoft grade (hardness 72 shore A) Modified 2533SN01 Applications: sport (tennis shoes parts)ISO data provided by the manufacturer, Arkema. |
|||
Surface Resistance | 3.00e+12 ohm | 3.00e+12 ohm | |
Arkema Group Pebax® 5533 SN 01 Polyether Block Amide (PEBA) (Conditioned) POLYETHER BLOCK AMIDE(PEBA) hardness 55 shore D Non plasticized flexible Polyamide Outstanding mechanical properties at low temperature (-40°C) Applications: overmolded parts for sport good (Footba.. |
|||
Surface Resistance | 3.00e+12 ohm | 3.00e+12 ohm | |
Covestro Desmopan® 453 Urethane Thermoplastic Elastomer
(discontinued **) Key Features:UnfilledSuitable processing methods:Injection moldingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially .. |
|||
Surface Resistance | 3.00e+12 ohm @Temperature 20.0 °C |
3.00e+12 ohm @Temperature 68.0 °F |
65% RH; ASTM D257 |
Arkema Group Pebax® MX 1205 Polyether Block Amide (PEBA) Typical application: Impact modifierInformation provided by Arkema Group |